MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crucible Steel KAPSTAR® Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Kapstar is a high hard, precipitation hardening mold steel suitable for production of machined or EDM’d plastic mold, rubber mold, and zinc die casting die components. Kapstar is supplied at about 40 HRC and further heat treating is generally not required. It is a through-hardened steel that exhibits uniform hardness through thick and thin sections. It is easily machined, polished, textured, and welded.

Information provided by Crucible Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.282 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 32 - 42
Modulus of Elasticity 29900 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.10 µin/in-°F
@Temperature 21.1 - 100 °C
 6.20 µin/in-°F
@Temperature 21.1 - 200 °C
 7.00 µin/in-°F
@Temperature 21.1 - 300 °C
 7.50 µin/in-°F
@Temperature 21.1 - 400 °C
Thermal Conductivity 182 BTU-in/hr-ft²-°F
@Temperature 21.1 °C
 194 BTU-in/hr-ft²-°F
@Temperature 100 °C
 203 BTU-in/hr-ft²-°F
@Temperature 200 °C
 217 BTU-in/hr-ft²-°F
@Temperature 300 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 1.0 %
Carbon, C 0.12 %
Chromium, Cr 0.50 %
Copper, Cu 0.20 %
Iron, Fe 91.8 %as balance
Manganese, Mn 1.5 %
Molybdenum, Mo 0.25 %
Nickel, Ni 4.0 %
Silicon, Si 0.40 %
Sulfur, S 0.10 %
Vanadium, V 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe Lesco 53 VIM-VAR Premium Carburizing Steel
Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures
HY-80 Steel
HY-100 Steel
EOS MS1 Maraging Steel Sintered on EOSINT M 270

NCRUC942 / 160393

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.