MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Latrobe Lesco 53 VIM-VAR Premium Carburizing Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel

Material Notes: LESCO 53 VIM-VAR is a premium quality alloy carburizing gear steel designed to resist softening at elevated service temperatures. It is double vacuum processed by vacuum induction melting followed by vacuum arc remelting to provide optimum metallurgical quality. Based on its combination of high-temperature performance, deep hardenability, and excellent toughness and fatigue resistance, Lesco 53 VIM-VAR find application in demanding helicopter and aerospace drive train components.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 3535Core between 70°F and 600°F
 5555Case at 600°C
Tensile Strength, Ultimate 1170 MPa170000 psi
Tensile Strength, Yield 965 MPa140000 psi
Elongation at Break 16 %16 %in 2"
Reduction of Area 63.5 %63.5 %
Charpy Impact 118 - 129 J87.0 - 95.1 ft-lbV-Notch
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.26 µm/m-°C
@Temperature 24.0 - 93.0 °C
6.256 µin/in-°F
@Temperature 75.2 - 199 °F
 12.25 µm/m-°C
@Temperature 24.0 - 316 °C
6.806 µin/in-°F
@Temperature 75.2 - 601 °F
 13.05 µm/m-°C
@Temperature 24.0 - 538 °C
7.250 µin/in-°F
@Temperature 75.2 - 1000 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.11 %0.11 %
Chromium, Cr 1.0 %1.0 %
Copper, Cu 2.0 %2.0 %
Iron, Fe 90.24 %90.24 %
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 3.25 %3.25 %
Nickel, Ni 2.0 %2.0 %
Silicon, Si 0.90 %0.90 %
Vanadium, V 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 6118H Steel
ASTM A514 Steel, grade D, plate thickness ≤ 19 mm
ASTM A871 HSLA Steel Grade 60, Hot-Rolled, 5-35 mm (3/16 to 1 3/8 in.)
Bisalloy Steels BisPlate 450 Thickness 8-20 mm
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties

NTIMK003 / 19351

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.