MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

HY-80 Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: This quenched and tempered low-carbon alloy steel finds uses as pressure vessels, heavy construction equipment, and in large steel structures. It has high tensile strength (yield and ultimate), good ductility, notch toughness, atmospheric corrosion resistance, and weldability.

Key Words: HY80
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 552 MPa>= 80000 psi
Elongation at Break 17 - 20 %17 - 20 %
Modulus of Elasticity 205 GPa29700 ksiTypical of steel
Poissons Ratio 0.280.28Calculated
Shear Modulus 80.0 GPa11600 ksiTypical of steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.12 - 0.18 %0.12 - 0.18 %
Chromium, Cr 1.0 - 1.8 %1.0 - 1.8 %
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe 93.1 - 96.4 %93.1 - 96.4 %As Balance
Manganese, Mn 0.10 - 0.40 %0.10 - 0.40 %
Molybdenum, Mo 0.20 - 0.60 %0.20 - 0.60 %
Nickel, Ni 2.0 - 3.25 %2.0 - 3.25 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.025 %<= 0.025 %
Titanium, Ti <= 0.020 %<= 0.020 %
Vanadium, V <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
HY-100 Steel
China Tungsten YG15 Tungsten Carbide Powder
HY-130 Steel
ASTM A812 HSLA Steel Grade 65 Sheet
Overview of materials for AISI 4000 Series Steel

MSHY80 / 14080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.