MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Xantar® 24UR Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: XANTAR® Polycarbonate is a versatile thermoplastic resin that is suitable for a wide range of applications and can be converted using all common melt-processing techniques. The XANTAR® product line consists of general purpose and special grades

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Melt Density 1.01 g/cc
@Temperature 300 °C
0.0365 lb/in³
@Temperature 572 °F
Water Absorption 0.35 %0.35 %Sim. To ISO 62
Viscosity Number 52 cm³/g0.52 dl/gLimiting Viscosity Number; ISO 1628-4
 58 cm³/g0.58 dl/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inISO 294-4
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiISO-527-1,2
Elongation at Break >= 50 %>= 50 %ISO 527-1,2
Elongation at Yield 6.0 %6.0 %ISO 527-1,2
Tensile Modulus 2.30 GPa334 ksiISO 527-1,2
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 2.40 GPa348 ksiISO 178
Izod Impact, Notched (ISO) 80.0 kJ/m²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 180/4A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 29.0 kV/mm737 kV/inIEC 60243-1
Dissipation Factor  0.00066
@Frequency 100 Hz
0.00066
@Frequency 100 Hz
IEC 60250
 0.0092
@Frequency 1e+6 Hz
0.0092
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 V225 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C36.1 µin/in-°FISO 11359,1-2
Specific Heat Capacity 1.71 J/g-°C0.409 BTU/lb-°Fmelt
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°Fmelt
Hot Ball Pressure Test 125 °C257 °FIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °FISO 75-1,2
Vicat Softening Point 150 °C
@Load 5.10 kg
302 °F
@Load 11.2 lb
rate 50°C/h; ISO 306
UL RTI, Electrical  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical with Impact  125 °C
@Thickness 0.750 mm
257 °F
@Thickness 0.0295 in
UL 746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical without Impact  125 °C
@Thickness 0.750 mm
257 °F
@Thickness 0.0295 in
UL 746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746B
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
IEC 60695, 11-10
 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
IEC 60695, 11-10
Oxygen Index 26 %26 %ISO 4589, 1-2
Glow Wire Ignition Temperature  825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
 875 °C
@Thickness 3.00 mm
1610 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  800 °C
@Thickness 1.50 mm
1470 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 89 %89 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 °C572 °FAs Tested; Injection; ISO 294
Mold Temperature 90.0 °C194 °FAs Tested; Injection; ISO 10724
Ejection Temperature 131 °C268 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Xantar® XRM 1006 Polycarbonate
Mitsubishi Xantar® MX 1021 FD MX 1021 Polycarbonate
Mitsubishi Xantar® MX 1020 Polycarbonate
Mitsubishi Xantar® F 23 R Polycarbonate
Mitsubishi Xantar® 22 R Polycarbonate

PMITSU9349 / 192013

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.