MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mitsubishi Xantar® MX 1020 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances where quality is a key requirement. The Xantar® range includes:
  • clear and tinted grades for transparent applications
  • reinforced materials
  • Flame retardant and halogen free types
  • lubricated materials for added wear resistance

Mitsubishi Engineering Plastics acquired the Xantar® product line from DSM in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Water Absorption 0.35 %0.35 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inISO 294-4
Melt Flow 7.08 g/10 min
@Load 1.20 kg,
Temperature 280 °C
7.08 g/10 min
@Load 2.65 lb,
Temperature 536 °F
Calculated from Volume Flow Rate of 6 cm3/10min.; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 52.0 MPa7540 psiISO 527-1/-2
Elongation at Break >= 50 %>= 50 %ISO 527-1/-2
Elongation at Yield 6.0 %6.0 %ISO 527-1/-2
Tensile Modulus 2.10 GPa305 ksiISO 527-1/-2
Flexural Strength 80.0 MPa11600 psiISO 178
Flexural Modulus 2.20 GPa319 ksiISO 178
Izod Impact, Notched (ISO)  60.0 kJ/m²
@Temperature -20.0 °C
28.6 ft-lb/in²
@Temperature -4.00 °F
ISO 180/4A
 70.0 kJ/m²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 180/4A
Dart Drop, Total Energy  11.0 J
@Temperature -30.0 °C
8.11 ft-lb
@Temperature -22.0 °F
Puncture Energy; ISO 6603-2
 16.0 J
@Temperature 23.0 °C
11.8 ft-lb
@Temperature 73.4 °F
Puncture Energy; ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243-1
Comparative Tracking Index 250 - 399 V250 - 399 VPLC 2; UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 20.0 °C
36.1 µin/in-°F
@Temperature 68.0 °F
ISO 11359-1/-2
Maximum Service Temperature, Air 125 °C257 °FBall Pressure Temperature; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 129 °C264 °FISO 75-1/-2
Vicat Softening Point 140 °C284 °F50°C/h 50N; ISO 306
 
Descriptive Properties
High Impact or Impact ModifiedYes
Injection MoldingYes
Release AgentYes
Without FillersYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2258 Polycarbonate
Chi Mei Wonderlite® PC-175 Polycarbonate
Kingfa JH820 Modified PC
EMS-Griltech Grilamid® HP 1200 Nylon 12 Fiber (Staple Length = 43)
EMS-Griltech Grilamid® DM 10 Nylon 12 Monofilament

PDSMEU660 / 31451

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.