MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Wonderlite® PC-175 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Optical Disk

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Melt Flow 65 g/10 min
@Load 1.20 kg,
Temperature 300 °C
65 g/10 min
@Load 2.65 lb,
Temperature 572 °F
Melt Volume Rate (ml/10 min); ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 106 MPa15400 psiH358/30; ISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527
Elongation at Break 65 %65 %50 mm/min; ISO 527
Flexural Strength 90.0 MPa13100 psi2 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180/4A
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 124 °C255 °Fannealed; ISO 75
 140 °C284 °Funannealed; ISO 75
Vicat Softening Point  140 °C
@Load 5.00 kg
284 °F
@Load 11.0 lb
50°C/hr; ISO 306
 145 °C
@Load 1.00 kg
293 °F
@Load 2.20 lb
50°C/hr; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Wonderlite® PC-115 Polycarbonate
Chi Mei Wonderlite® PC-110 Polycarbonate
Chi Mei Wonderlite® PC-122 Polycarbonate
Chi Mei Wonderlite® PC-110V Polycarbonate - Flame Retardant
Chi Mei Wonderloy® PC-345 PC/ABS Alloy

PCHI952 / 109440

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.