MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Xantar® XRM 1006 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Impact modified flame retardant PC. This naturally bright white grade can be colored easily and exhibits a unique combination of properties, exceeding those of conventional PC and PC/ABS grades: No plasticizing effect, high ultimate temperature use, equal to PC. Excellent low temperature impact, down to e.g. -40ºC. Outstanding dimensional stability, excellent creep behavior. UL94 V-1, V-0 and 5V flammability ratings, offering security to applications. Excellent electrical performance, e.g. CTI PLC 2, HWI and HAI both PLC 0 ! Excellent environmental stress cracking resistance, outperforming even the most robust PC/ABS grades. Easy processing, no juicing or outgassing. Free of chlorine, bromine, phosphorous and antimony, enhancing the green image of its applications, and is available in both reinforced and non-reinforced grades.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Melt Density 1.04 g/cc
@Temperature 290 °C
0.0376 lb/in³
@Temperature 554 °F
Water Absorption 0.35 %0.35 %
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/in
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
cm³/10 min Volumetric Rate
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 6.0 %6.0 %
Tensile Modulus 2.20 GPa319 ksi
Flexural Strength 80.0 MPa11600 psi
Flexural Modulus 2.30 GPa334 ksi
Izod Impact, Notched (ISO)  30.0 kJ/m²
@Temperature -40.0 °C
14.3 ft-lb/in²
@Temperature -40.0 °F
 60.0 kJ/m²
@Temperature -20.0 °C
28.6 ft-lb/in²
@Temperature -4.00 °F
 70.0 kJ/m²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
Impact  <= 5500
@Temperature 23.0 °C
<= 5500
@Temperature 73.4 °F
N; Puncture - Max Force
 <= 6000
@Temperature -30.0 °C
<= 6000
@Temperature -22.0 °F
N; Puncture - Max Force
Puncture Energy 60.0 J44.3 ft-lb
 60.0 J44.3 ft-lb
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm1.00e+15 ohm
Dielectric Constant  2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
Dielectric Strength 29.0 kV/mm737 kV/in
Dissipation Factor  0.00066
@Frequency 100 Hz
0.00066
@Frequency 100 Hz
 0.0092
@Frequency 1e+6 Hz
0.0092
@Frequency 1e+6 Hz
Comparative Tracking Index 200 V200 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C36.1 µin/in-°F
Specific Heat Capacity 2.15 J/g-°C0.514 BTU/lb-°Fmelt
Thermal Conductivity 0.260 W/m-K1.80 BTU-in/hr-ft²-°Fmelt
Hot Ball Pressure Test 140 °C284 °F
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °F
Vicat Softening Point 145 °C
@Load 5.10 kg
293 °F
@Load 11.2 lb
rate 50°C/h
Flammability, UL94  V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
 V-0
@Thickness 2.50 mm
V-0
@Thickness 0.0984 in
 5VB
@Thickness 2.50 mm
5VB
@Thickness 0.0984 in
Oxygen Index 28 %28 %
Glow Wire Ignition Temperature  850 °C
@Thickness 2.00 mm
1560 °F
@Thickness 0.0787 in
 875 °C
@Thickness 3.00 mm
1610 °F
@Thickness 0.118 in
Glow Wire Flammability Index  960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °FAs Tested; Injection
Mold Temperature 80.0 °C176 °FAs Tested; Injection
Ejection Temperature 144 °C291 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omni Plastics OmniCarb™ PC/ABS 20 FR PC/ABS
A. Schulman Diamond NPP 808 C3 TDS Polycarbonate Alloy
Mitsubishi Iupilon® GPX 2010PH Polycarbonate
Mitsubishi Xantar® E EM 605 Polycarbonate
Mitsubishi Xantar® MX 1001 Polycarbonate

PMITSU9308 / 191982

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.