MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Xantar® XRM 1006 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Impact modified flame retardant PC. This naturally bright white grade can be colored easily and exhibits a unique combination of properties, exceeding those of conventional PC and PC/ABS grades: No plasticizing effect, high ultimate temperature use, equal to PC. Excellent low temperature impact, down to e.g. -40ºC. Outstanding dimensional stability, excellent creep behavior. UL94 V-1, V-0 and 5V flammability ratings, offering security to applications. Excellent electrical performance, e.g. CTI PLC 2, HWI and HAI both PLC 0 ! Excellent environmental stress cracking resistance, outperforming even the most robust PC/ABS grades. Easy processing, no juicing or outgassing. Free of chlorine, bromine, phosphorous and antimony, enhancing the green image of its applications, and is available in both reinforced and non-reinforced grades.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Melt Density 1.04 g/cc
@Temperature 290 °C
Water Absorption 0.35 %
Linear Mold Shrinkage, Flow 0.0080 cm/cm
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min Volumetric Rate
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPa
Elongation at Break >= 50 %
Elongation at Yield 6.0 %
Tensile Modulus 2200 MPa
Flexural Strength 80.0 MPa
Flexural Modulus 2300 MPa
Izod Impact, Notched (ISO) 30.0 kJ/m²
@Temperature -40.0 °C
 60.0 kJ/m²
@Temperature -20.0 °C
 70.0 kJ/m²
@Temperature 23.0 °C
Impact <= 5500
@Temperature 23.0 °C
N; Puncture - Max Force
 <= 6000
@Temperature -30.0 °C
N; Puncture - Max Force
Puncture Energy 60.0 J
 60.0 J
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
Dielectric Constant 2.8
@Frequency 1e+6 Hz
 2.9
@Frequency 100 Hz
Dielectric Strength 29.0 kV/mm
Dissipation Factor 0.00066
@Frequency 100 Hz
 0.0092
@Frequency 1e+6 Hz
Comparative Tracking Index 200 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
Specific Heat Capacity 2.15 J/g-°Cmelt
Thermal Conductivity 0.260 W/m-Kmelt
Hot Ball Pressure Test 140 °C
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
Vicat Softening Point 145 °C
@Load 5.10 kg
rate 50°C/h
Flammability, UL94 V-1
@Thickness 1.50 mm
 V-0
@Thickness 2.50 mm
 5VB
@Thickness 2.50 mm
Oxygen Index 28 %
Glow Wire Ignition Temperature 850 °C
@Thickness 2.00 mm
 875 °C
@Thickness 3.00 mm
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
 960 °C
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °CAs Tested; Injection
Mold Temperature 80.0 °CAs Tested; Injection
Ejection Temperature 144 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omni Plastics OmniCarb™ PC/ABS 20 FR PC/ABS
A. Schulman Diamond NPP 808 C3 TDS Polycarbonate Alloy
Mitsubishi Iupilon® GPX 2010PH Polycarbonate
Mitsubishi Xantar® E EM 605 Polycarbonate
Mitsubishi Xantar® MX 1001 Polycarbonate

PMITSU9308 / 191982

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.