MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Xantar® E EM 605 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: Polycarbonate + Polyethylene Terephthalate. XANTAR® E (PC/Polyester blends) combines outstanding ductility at very low temperatures and very low emission of volatiles. For this reason it has been successfully used in very critical automotive interior applications.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Water Absorption 0.35 %0.35 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/inISO 294-4
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 280 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 536 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psiISO 527-1/-2
Elongation at Break >= 50 %>= 50 %ISO 527-1,2
Elongation at Yield 6.0 %6.0 %ISO 527-1,2
Tensile Modulus 2.20 GPa319 ksiISO 527-1,2
Flexural Strength 80.0 MPa11600 psiISO 178
Flexural Modulus 2.20 GPa319 ksiISO 178
Izod Impact, Notched (ISO)  40.0 kJ/m²
@Temperature -40.0 °C
19.0 ft-lb/in²
@Temperature -40.0 °F
ISO 180/4A
 60.0 kJ/m²
@Temperature -20.0 °C
28.6 ft-lb/in²
@Temperature -4.00 °F
ISO 180/4A
 70.0 kJ/m²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 180/4A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359-1-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359-1-2
Thermal Conductivity 0.162 W/m-K1.12 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FISO 75-1,2
Vicat Softening Point 130 °C
@Load 5.10 kg
266 °F
@Load 11.2 lb
rate 50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond NPP 808 C3 TDS Polycarbonate Alloy
Mitsubishi Iupilon® GPX 2010PH Polycarbonate
Mitsubishi Xantar® MX 1002 Polycarbonate
Mitsubishi Xantar® MX 1001 Polycarbonate
Mitsubishi Xantar® XRM 1006 Polycarbonate

PMITSU9013 / 191686

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.