MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ArcelorMittal Save 30-17 Electrical Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencies.

Advantages: Save grades enable you to reduce the iron losses from the stators of synchronous machines. They are particularly useful for reducing iron losses in high-speed hybrid and electric traction machines, and generators which extend the range of electric vehicles.

Applications: Save grades are most effective at reducing iron losses from machine parts which are subject to high base frequencies and additional harmonics. Save thus helps to improve machine efficiency, which leads to an increase in power density. Power density can be tuned to create a lighter, smaller machine, or a more powerful machine for a given weight. Driving range is extended as Save reduces machine weight and costs and saves battery energy.

Recommendations for use: Save grades can be used immediately after lamination punching. The punching effect can be eliminated by performing a stress relief annealing. This optimises their performance in applications with fine teeth, and enables a substantial part of the lower frequency area to be exploited. A C5-type coating is recommended. Save stacks can be produced using existing assembly techniques such as interlocking or welding.

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.60 g/cc0.275 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 195 - 225195 - 225L direction
 195 - 225195 - 225T direction
Tensile Strength, Ultimate 510 - 550 MPa74000 - 79800 psiL direction
 540 - 580 MPa78300 - 84100 psiT direction
Tensile Strength, Yield 390 - 430 MPa56600 - 62400 psiL direction
 410 - 450 MPa59500 - 65300 psiT direction
Elongation at Break 15 - 30 %15 - 30 %L direction
 15 - 30 %15 - 30 %T direction
 
Magnetic PropertiesMetricEnglishComments
Core Loss  <= 17.0 W/kg
@Frequency 400 Hz
<= 7.71 W/lb
@Frequency 400 Hz
at 1T, Guaranteed
 <= 41.0 W/kg
@Frequency 700 Hz
<= 18.6 W/lb
@Frequency 700 Hz
at 1T, Indicative
 
Descriptive Properties
Anisotropy>15%400 Hz at 1T
Polarization>1.49 Tat 2,500 A/m
 >1.6 Tat 5,000 A/m
 >1.7 Tat 10,000 A/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel (Extended Electrical/Magnetic Data)
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel
ArcelorMittal Save 20-13 Electrical Steel
ArcelorMittal Torque 30-17 Electrical Steel
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel

NARCE116 / 160024

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.