MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for lower core losses and less noisy transformer core structures, particularly at higher operating inductions, when compared to conventional grain oriented electrical steels. The core loss characteristics are further enhanced in the TRAN-COR H CARLITE DR® (Domain Refined) products where laser scribing is employed. In this process, a precisely focused laser beam is rapidly scanned across the steel surface. The micro-strain imparted into the material forces the pre-existing magnetic domains to subdivide. The finer domain structure reduces the distance that the domain walls must move during AC magnetization, thereby reducing eddy current losses. The result is far lower core loss than possible with conventional grain oriented electrical steels of comparable thickness. TRAN-COR H CARLITE products are suitable for all types of transformers while TRAN-COR H DR products are suitable for those types of transformers where a stress relief annealing treatment of the magnetic core is not used. Stress relief annealing will result in the eradication of the effect provided by the laser treatment and will result in a significant increase in core loss.

Information provided by AK Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.65 g/cc0.276 lb/in³
Thickness 200 - 240 microns7.87 - 9.45 mil
 230 microns9.06 milNominal
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 173173
Hardness, Rockwell B 8383
Tensile Strength, Ultimate 359 MPa52100 psiIn rolling direction
Tensile Strength, Yield 345 MPa50000 psiIn rolling direction
Elongation at Break 11 %11 %In 2", rolling direction
Modulus of Elasticity 113.8 GPa16510 ksiIn rolling direction
 138 GPa20000 ksiAt 20° to rolling direction
 203 GPa29400 ksiAt 90° to rolling direction
 241 GPa35000 ksiAt 45° to rolling direction
 276 GPa40000 ksiAt 55° to rolling direction
 
Electrical PropertiesMetricEnglishComments
Exciting Power (RMS)  0.00183 RMS AT/cm
@Magnetic Field 0.100 T,
Frequency 50 Hz
0.00290 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A804, 0.23 mm
 3.0456 RMS AT/cm
@Magnetic Field 1.90 T,
Frequency 60 Hz
4.8136 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
ASTM A804, 0.23 mm
Electrical Resistivity 0.0000500 ohm-cm0.0000500 ohm-cm
 
Magnetic PropertiesMetricEnglishComments
Core Loss  0.00326 W/kg
@Magnetic Field 0.100 T,
Frequency 50 Hz
0.00148 W/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A804, 0.23 mm
 2.05 W/kg
@Magnetic Field 1.90 T,
Frequency 60 Hz
0.930 W/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
ASTM A343, 0.23 mm
 
Descriptive Properties
Approximate Equivalent International GradeM090-23P5
Magnetostriction 10^8-32ASTM A876, 1.4T, 60Hz, 0.23 mm
 -37ASTM A876, 1.5T, 60Hz, 0.23 mm
 -40ASTM A876, 1.6T, 60Hz, 0.23 mm
 -44ASTM A876, 1.7T, 60Hz, 0.23 mm
Maximum Induction at 800 A/m (T)1.88
Minimum Lamination Factor (%)94.5
Typical Induction at 800 A/m (T)1.917
Typical Lamination Factor (%)96.6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel (Extended Electrical/Magnetic Data)
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel
AK Steel CARLITE® M-3 Grain Oriented Electrical Steel
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel (Extended Electro-Magnetic Data)

NAKS163a / 140759

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.