MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Materion Alloy 390E Copper Beryllium Strip
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Alloy 390E is a copper beryllium alloy that provides a unique combination of high strength, high electrical conductivity, and excellent formability. Copper beryllium alloys are well known for their superior stress relaxation resistance and fatigue strength. This allows engineers the flexibility to design small form factor signal and power interconnects that can be used in harsh environments.

Information supplied by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.83 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell >= 300DPH
Tensile Strength, Ultimate >= 986 MPa
Tensile Strength, Yield >= 951 MPa
@Strain 0.2 %
Elongation at Break >= 2.0 %
@Thickness >=0.100 mm
Creep Strength 492 MPa
@Temperature 200 °C,
Time 3.60e+6 sec
Initial stress = 713 MPa (69% retained)
 606 MPa
@Temperature 150 °C,
Time 3.60e+6 sec
Initial stress = 713 MPa (85% retained)
Modulus of Elasticity 138 GPa
Fatigue Strength 552 MPa
@Thickness >=0.100 mm,
# of Cycles 1.00e+7
R=0
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 0.00000374 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.6 µm/m-°C
Specific Heat Capacity 0.419 J/g-°C
Thermal Conductivity 208 W/m-K
Melting Point >= 1029 °C
Solidus 1029 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam Invar® FeNi36 Bar-Corrosion application
UNS C81400, Copper Casting Alloy
Beryllium Copper, UNS C17200, TF00 Temper rod, bar, plate, tubing
Beryllium Copper, UNS C17200, TH04 Temper rod, bar, plate, tubing, >25 mm
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets

NBB699 / 192243

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.