MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aperam Invar® FeNi36 Bar-Corrosion application
Categories: Metal; Ferrous Metal

Material Notes: This grade is a nickel-iron with very low thermal expansion from cryogenic temperatures up to 200°C.

Applications:

  • Aeronautic Mould, missile body
  • Liquid gas transport, cryogeny
  • Optical device, Space and detection devices
Standards related to these applications: ASTM F1684 – SEW 385 – A54-301

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.10 µm/m-°C
@Temperature 0.000 - 100 °C
0.611 µin/in-°F
@Temperature 32.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 63 - 65 %63 - 65 %
Nickel, Ni 35 - 37 %35 - 37 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Invar 36® Alloy, Cold Drawn Bars
Carpenter Invar 36® Alloy, Annealed Bars and Strip
Carpenter Invar 36® Alloy, Cold Rolled Strip
Aperam Invar® FeNi336 Cold Rolled Strip
Carpenter Super Invar 32-5

NPERA039 / 194828

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.