MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Materion Alloy 390E Copper Beryllium Strip
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Alloy 390E is a copper beryllium alloy that provides a unique combination of high strength, high electrical conductivity, and excellent formability. Copper beryllium alloys are well known for their superior stress relaxation resistance and fatigue strength. This allows engineers the flexibility to design small form factor signal and power interconnects that can be used in harsh environments.

Information supplied by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell >= 300>= 300DPH
Tensile Strength, Ultimate >= 986 MPa>= 143000 psi
Tensile Strength, Yield >= 951 MPa
@Strain 0.2 %
>= 138000 psi
@Strain 0.2 %
Elongation at Break >= 2.0 %
@Thickness >=0.100 mm
>= 2.0 %
@Thickness >=0.00394 in
Creep Strength  492 MPa
@Temperature 200 °C,
Time 3.60e+6 sec
71400 psi
@Temperature 392 °F,
Time 1000 hour
Initial stress = 713 MPa (69% retained)
 606 MPa
@Temperature 150 °C,
Time 3.60e+6 sec
87900 psi
@Temperature 302 °F,
Time 1000 hour
Initial stress = 713 MPa (85% retained)
Modulus of Elasticity 138 GPa20000 ksi
Fatigue Strength 552 MPa
@Thickness >=0.100 mm,
# of Cycles 1.00e+7
80100 psi
@Thickness >=0.00394 in,
# of Cycles 1.00e+7
R=0
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00000374 ohm-cm<= 0.00000374 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C9.78 µin/in-°F
Specific Heat Capacity 0.419 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 208 W/m-K1440 BTU-in/hr-ft²-°F
Melting Point >= 1029 °C>= 1884 °F
Solidus 1029 °C1884 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aperam Invar® FeNi36 Bar-Corrosion application
UNS C81400, Copper Casting Alloy
Beryllium Copper, UNS C17200, TF00 Temper rod, bar, plate, tubing
Beryllium Copper, UNS C17200, TH04 Temper rod, bar, plate, tubing, >25 mm
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets

NBB699 / 192243

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.