MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive, Flexible

Material Notes: Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some plastics and rubbers. Epovex Paste was also designed to bond Zyvex Technologies’ Arovex® composites.

Features:

  • Excellent flexibility
  • Very high T-peel strengths
  • Very high tensile shear strengths
  • Non-drop, non-sag on vertical surfaces

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccPart B
 1.28 g/ccPart A
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 1300 psi
@Temperature 82.2 °C
Cure cycle: 7 days @ RT , with Aced Etched 6061-T6 Aluminum
 1750 psi
@Temperature 60.0 °C
Arovex (abraded), with Arovex Carbon Fiber Epoxy Laminate
 2210 psi
@Temperature 60.0 °C
Aluminum (abraded), with Arovex Carbon Fiber Epoxy Laminate
 2600 psi
@Temperature 60.0 °C
Cure cycle: 7 days @ RT , with Aced Etched 6061-T6 Aluminum
 3100 psi
@Temperature 23.9 °C
Cure cycle: 7 days @ RT (+7 days ethyl alcohol soak), with Aced Etched 6061-T6 Aluminum
 3100 psi
@Temperature 23.9 °C
Cure cycle: 7 days @ RT (+7 days gasoline soak) , with Aced Etched 6061-T6 Aluminum
 3440 psi
@Temperature 23.9 °C
Arovex (abraded), with Arovex Carbon Fiber Epoxy Laminate
 3500 psi
@Temperature 23.9 °C
Aluminum (abraded), with Arovex Carbon Fiber Epoxy Laminate
 3600 psi
@Temperature 23.9 °C
Cure cycle: 7 days @ RT (+7 days water soak) , with Aced Etched 6061-T6 Aluminum
 3700 psi
@Temperature 23.9 °C
Arovex (abraded) (+7 days water soak), with Arovex Carbon Fiber Epoxy Laminate
 3700 psi
@Temperature 23.9 °C
Cure cycle: 3 days @ RT, with Aced Etched 6061-T6 Aluminum
 4000 psi
@Temperature 23.9 °C
Cure cycle: 7 days @ RT, with Aced Etched 6061-T6 Aluminum
 4000 psi
@Temperature 23.9 °C
Cure cycle: 12 hrs @ RT + 1 hr @ 176°F, with Aced Etched 6061-T6 Aluminum
 4400 psi
@Temperature 23.9 °C
Cure cycle: 2 hrs @ 176°F, with Aced Etched 6061-T6 Aluminum
 4400 psi
@Temperature -40.0 °C
Cure cycle: 7 days @ RT , with Aced Etched 6061-T6 Aluminum
Peel Strength 30.0 pliCure cycle: 1 day @ RT, with Acid Etched 6061-T6 Aluminum
 35.0 pliCure cycle: 3 days @ RT, with Acid Etched 6061-T6 Aluminum
 40.0 pliCure cycle: 12 hrs @ RT + 1 hr @ 176°F, with Acid Etched 6061-T6 Aluminum
 
Descriptive Properties
ColorAmberPart B, uncured
 BlackBlend, uncured
 BlackPart A, uncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
1,3-Butanediol, C4H10O2
Nanocyl EPOCYL™ NC R128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes: Dilution Factor 6
Overview of materials for Epoxy/Carbon Fiber Composite
Solvay Thornel® VCL Carbon Cloth Laminate with Mil R-9299 Resin
Nanocyl EPOCYL™ NC E128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes

PZYVEX92B / 159345

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.