MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Solvay Thornel® VCL Carbon Cloth Laminate with Mil R-9299 Resin
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite; Filled/Reinforced Thermoset

Material Notes: Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperatures to yield products with a high degree of purity. The cloth flexibility results from the very small filament diameter. These are fair conductors of electricity. At room temperature the volume resistivity of graphite cloth is about 40 times that of "Nichrome" wire. Graphite cloth resistance decreases with temperature, reaching half of the room temperature value at 1315°C.

Cloth carbon assay is 97%. Filament diameter is 8.9 µm.

Solvay has acquired the Thornel product line as a part of the Cytec purchase.

Key Words: Carbon Fibre
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Cloth 1.75 g/cc per He measurement
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 6565
Tensile Strength, Ultimate 110 MPa16000 psi
Tensile Modulus 15.0 GPa2180 ksi
Flexural Yield Strength 170 MPa24700 psi
Flexural Modulus 14.0 GPa2030 ksi
Compressive Yield Strength 165 MPa23900 psi
Compressive Modulus 11.0 GPa1600 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 °C
7.78 µin/in-°F
@Temperature 68.0 °F
Warp
Specific Heat Capacity 1.20 J/g-°C0.287 BTU/lb-°F
Thermal Conductivity 6.00 W/m-K41.6 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy/Carbon Fiber Composite
Solvay Thornel® VCK Carbon Cloth Laminate with Mil R-9299 Resin
Arlon Electronic Materials 45NK Woven Kevlar® Reinforced Laminate and Prepreg
Solvay Thornel® Graphite Cloth Laminate with Mil R-9299 Resin
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System

PCYTEC701 / 21387

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.