MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

1,3-Butanediol, C4H10O2
Categories: Fluid; Solvent

Key Words: C4H10O2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc
@Temperature 20.0 °C
0.0361 lb/in³
@Temperature 68.0 °F
Viscosity 98.3 cP
@Temperature 20.0 °C
98.3 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 90.12 g/mol90.12 g/mol
Surface Tension 37.8 dynes/cm
@Temperature 20.0 °C
37.8 dynes/cm
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 28.8
@Temperature 20.0 °C
28.8
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.1844 W/m-K
@Temperature 20.0 °C
1.280 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -77.0 °C-107 °F
Boiling Point 207.5 °C405.5 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.44
@Wavelength 589.3 nm
1.44
@Wavelength 589.3 nm
nD
 
Descriptive Properties
CAS registry number (CARN)107-88-0
Chemical FormulaC4H10O2
Henry's Law Constant (atm m3/mol)2.304E-07

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste
Diamond, Natural
American Chestnut Wood
American Black Gum (Black Tupelo) Wood
American Black Ash (Brown Ash) Wood

VORGS036 / 99426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.