MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CIP Composites 300 Series Laminated Polymer Bearing Material
Categories: Polymer; Thermoset

Material Notes: The 300 series consists of Nomex® fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated polymer material made by impregnating textile with a thermoset resin. CIP Composites™ offer design engineers an attractive, cost effective alternative to the traditional materials used for bushings, bearings, wear pads, and thrust washers, such as bronze, brass or nylon. CIP Composites™ are only 1/6 the weight of steel, easily machined, have good dimensional stability and do not contain harmful or toxic materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
@Temperature 20.0 - 204 °C
Parallel to Laminate
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature 20.0 - 204 °C
Normal to Laminate
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIP Composites 100 Series Laminated Polymer Bearing Material
CIP Composites 200 Series Laminated Polymer Bearing Material
Overview of materials for Brass
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, OSO25 Temper flat products, tube
Crucible Steel AISI 52100 Alloy Steel

PCIPC992 / 178364

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.