MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Brass
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Brass". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.969 - 8.89 g/cc0.0350 - 0.321 lb/in³Average value: 8.48 g/cc Grade Count:604
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 37.0 - 15537.0 - 155Average value: 81.3 Grade Count:29
Hardness, Rockwell B 12.0 - 13312.0 - 133Average value: 69.1 Grade Count:274
Hardness, Rockwell F 54.0 - 10054.0 - 100Average value: 68.9 Grade Count:94
Hardness, Rockwell 30T 8.00 - 2408.00 - 240Average value: 55.1 Grade Count:213
Hardness, Rockwell H 46.0 - 90.046.0 - 90.0Average value: 68.7 Grade Count:13
Hardness, Vickers 80.0 - 14080.0 - 140Average value: 105 Grade Count:4
Tensile Strength, Ultimate 20.7 - 1030 MPa3000 - 150000 psiAverage value: 411 MPa Grade Count:606
Tensile Strength, Yield 34.5 - 683 MPa5000 - 99100 psiAverage value: 253 MPa Grade Count:546
Elongation at Break 1.00 - 68.0 %1.00 - 68.0 %Average value: 28.8 % Grade Count:598
Reduction of Area 40.0 - 60.0 %40.0 - 60.0 %Average value: 52.4 % Grade Count:59
Modulus of Elasticity 75.8 - 121 GPa11000 - 17600 ksiAverage value: 105 GPa Grade Count:555
Compressive Yield Strength 62.1 - 2580 MPa9000 - 375000 psiAverage value: 384 MPa Grade Count:11
Poissons Ratio 0.260 - 0.4600.260 - 0.460Average value: 0.325 Grade Count:375
Fatigue Strength 22.0 - 360 MPa3190 - 52200 psiAverage value: 110 MPa Grade Count:107
Machinability 20.0 - 106 %20.0 - 106 %Average value: 50.0 % Grade Count:521
Shear Modulus 26.9 - 44.1 GPa3900 - 6400 ksiAverage value: 38.9 GPa Grade Count:421
Shear Strength 205 - 531 MPa29700 - 77000 psiAverage value: 274 MPa Grade Count:281
Izod Impact 10.8 - 45.0 J8.00 - 33.2 ft-lbAverage value: 38.7 J Grade Count:12
Charpy Impact 15.0 - 102 J11.1 - 75.0 ft-lbAverage value: 47.1 J Grade Count:52
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000318 - 0.0000860 ohm-cm0.00000318 - 0.0000860 ohm-cmAverage value: 0.00000818 ohm-cm Grade Count:542
Magnetic Permeability 1.00 - 4.951.00 - 4.95Average value: 1.33 Grade Count:25
Magnetic Susceptibility -1.00e-6-1.00e-6Average value: -1.00e-6 Grade Count:40
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 - 26.0 µm/m-°C10.0 - 14.4 µin/in-°FAverage value: 20.1 µm/m-°C Grade Count:334
Specific Heat Capacity 0.375 - 0.510 J/g-°C0.0896 - 0.122 BTU/lb-°FAverage value: 0.379 J/g-°C Grade Count:472
Thermal Conductivity 2.31 - 233 W/m-K16.0 - 1620 BTU-in/hr-ft²-°FAverage value: 85.1 W/m-K Grade Count:552
Melting Point 178 - 1090 °C353 - 2000 °FAverage value: 927 °C Grade Count:514
Solidus 178 - 1050 °C353 - 1920 °FAverage value: 911 °C Grade Count:509
Liquidus 843 - 1090 °C1550 - 2000 °FAverage value: 942 °C Grade Count:514
Annealing Point 427 - 760 °C800 - 1400 °FAverage value: 546 °C Grade Count:361
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 371 °C500 - 700 °FAverage value: 275 °C Grade Count:38
Annealing Temperature 425 - 750 °C797 - 1380 °FAverage value: 540 °C Grade Count:278
Hot-Working Temperature 625 - 950 °C1160 - 1740 °FAverage value: 769 °C Grade Count:376
Recrystallization Temperature 288 - 400 °C550 - 752 °FAverage value: 334 °C Grade Count:219
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.00500 - 3.00 %0.00500 - 3.00 %Average value: 0.542 % Grade Count:44
Antimony, Sb 0.0150 - 1.50 %0.0150 - 1.50 %Average value: 0.188 % Grade Count:49
Arsenic, As 0.0150 - 0.250 %0.0150 - 0.250 %Average value: 0.0756 % Grade Count:17
Bismuth, Bi 0.150 - 2.50 %0.150 - 2.50 %Average value: 1.14 % Grade Count:17
Boron, B 0.00200 - 0.200 %0.00200 - 0.200 %Average value: 0.143 % Grade Count:14
Cadmium, Cd 0.00100 - 0.0100 %0.00100 - 0.0100 %Average value: 0.00200 % Grade Count:9
Carbon, C 0.100 %0.100 %Average value: 0.100 % Grade Count:7
Copper, Cu 53.0 - 95.0 %53.0 - 95.0 %Average value: 69.4 % Grade Count:618
Iron, Fe 0.0500 - 3.00 %0.0500 - 3.00 %Average value: 0.193 % Grade Count:541
Lead, Pb 0.0200 - 11.0 %0.0200 - 11.0 %Average value: 0.811 % Grade Count:564
Manganese, Mn 0.0100 - 23.0 %0.0100 - 23.0 %Average value: 3.06 % Grade Count:59
Nickel, Ni 0.100 - 14.0 %0.100 - 14.0 %Average value: 1.79 % Grade Count:52
Phosphorus, P 0.0100 - 0.200 %0.0100 - 0.200 %Average value: 0.0659 % Grade Count:64
Selenium, Se 0.0100 - 1.10 %0.0100 - 1.10 %Average value: 0.518 % Grade Count:6
Silicon, Si 0.00500 - 5.50 %0.00500 - 5.50 %Average value: 1.21 % Grade Count:52
Sulfur, S 0.0500 - 0.650 %0.0500 - 0.650 %Average value: 0.201 % Grade Count:29
Tin, Sn 0.000 - 6.00 %0.000 - 6.00 %Average value: 1.10 % Grade Count:241
Titanium, Ti 0.100 - 0.300 %0.100 - 0.300 %Average value: 0.186 % Grade Count:7
Zinc, Zn 4.00 - 43.5 %4.00 - 43.5 %Average value: 28.8 % Grade Count:618
Zirconium, Zr 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.154 % Grade Count:13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Overview of materials for Bronze
Aluminum, Al
Overview of materials for Stainless Steel
Gilding Copper, UNS C21000, OSO50 Temper

M01052 / 81690

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.