MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CIP Composites 100 Series Laminated Polymer Bearing Material
Categories: Polymer; Thermoset

Material Notes: The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated polymer material made by impregnating textile with a thermoset resin. CIP Composites™ offer design engineers an attractive, cost effective alternative to the traditional materials used for bushings, bearings, wear pads, and thrust washers, such as bronze, brass or nylon. CIP Composites™ are only 1/6 the weight of steel, easily machined, have good dimensional stability and do not contain harmful or toxic materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Moisture Absorption <= 0.1 %<= 0.1 %water swell < 0.15%
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ASTM D785
Tensile Strength 75.8 MPa11000 psiASTM D638
Tensile Modulus 3.24 GPa470 ksiASTM D638
Flexural Modulus 1.79 GPa260 ksiASTM D790
Compressive Yield Strength 103 MPa15000 psiASTM D695
Compressive Strength 93.1 MPa13500 psiParallel to Laminate; ASTM D695
 345 MPa50000 psiASTM D695
Compressive Modulus 3.45 GPa500 ksiASTM D695
Poissons Ratio 0.2310.231ASTM D3039-08
Shear Strength 82.7 MPa12000 psiASTM D3846
Coefficient of Friction, Dynamic 0.13 - 0.150.13 - 0.15Dry, Grade CIP 151 (MoS2 + PTFE Filled)
 0.15 - 0.200.15 - 0.20Dry, Grade CIP 121 (Graphite Filled)
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.20e+15 ohm-cm4.20e+15 ohm-cmASTM D257-07
Dielectric Strength 7.87 kV/mm200 kV/inASTM D149-97a
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 32.0 µm/m-°C
@Temperature 20.0 - 93.3 °C
17.8 µin/in-°F
@Temperature 68.0 - 200 °F
Parallel to Laminate
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature 20.0 - 93.3 °C
35.0 µin/in-°F
@Temperature 68.0 - 200 °F
Normal to Laminate
Maximum Service Temperature, Air 93.3 °C200 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CIP Composites 200 Series Laminated Polymer Bearing Material
CIP Composites 300 Series Laminated Polymer Bearing Material
Garlock Viblon™ 256 Neoprene Bearing Pad
Overview of materials for Polyimide
Overview of materials for Bronze

PCIPC990 / 178347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.