MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: Low Compression Set

Use: Hydraulic Seals and Gaskets

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92 - 98
@Time 5.00 sec
ASTM D2240
Tensile Strength 33.9 MPaASTM D412
Elongation at Break 370 %ASTM D412/D638
100% Modulus 0.0135 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0250 GPa
@Strain 300 %
ASTM D412
Tear Strength 534 pliTrouser; ASTM D470
Graves Tear Strength 622 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 38H18, 1000g; ASTM D3389
Compression Set 23 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395 Method B
 37 %
@Temperature 100 °C,
Time 252000 sec
ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDSC
Glass Transition Temp, Tg -32.0 °CDSC
Shrinkage 0.0080 %
@Time 173000 sec
5" bark
 0.0080 %
@Time 173000 sec
4" disk
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 193 °CInjection
 216 °C
Middle Barrel Temperature 204 °CInjection
Nozzle Temperature 216 °CInjection
Melt Temperature 216 °CInjection
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
Injection Pressure 10000 - 15000 psiInjection
Hold Pressure 5000 - 10000 psiInjection
Back Pressure 50.0 psiInjection
Screw Speed 20 - 50 rpmInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® 58246 Thermoplastic Polyurethane
Lubrizol ESTANE® 58141 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane

PNOVEON028 / 55294

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.