MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58141 Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.

Benefits of Estane® TPU:

  • Outstanding Abrasion and Wear Resistance
  • Excellent Low Temperature Flexibility
  • Superior Toughness and Durability
  • Ease of Processing and Manufacturing Flexibility
  • Colorability and Paintability with no adhesion promoter
  • Applications:

    • Film & Sheet
    • Fabric coating & melt coating
    • Wire & Cable
    • Hose, Tube & Profile
    • Custom molding
    • Custom compounding
    • Automotive interior/chassis and exterior painted trim

    Information provided by Noveon, Inc.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.21 g/cc1.21 g/ccISO 2781
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 9696ISO 868
    Hardness, Shore D 4949ISO 868
    Tensile Strength, Ultimate 30.0 MPa4350 psiISO 37
    Elongation at Break 540 %540 %ISO 37
    Tensile Modulus 0.0880 GPa12.8 ksiISO 527
    50% Modulus 10.1 MPa
    @Strain 50 %
    10.1 MPa
    @Strain 50 %
    ISO 37
    100% Modulus 11.7 MPa
    @Strain 100 %
    1700 psi
    @Strain 100 %
    ISO 37
    300% Modulus 20.0 MPa
    @Strain 300 %
    2900 psi
    @Strain 300 %
    ISO 37
    Rebound 35 %35 %ISO 4662
    Tear Strength 100 kN/m571 pliwith incision; ISO 34B
     138 kN/m787 pliwithout incision; ISO 34B
    Abrasion 4545mm3; ISO 4649
    Compression Set  19 %
    @Temperature 22.0 °C,
    Time 252000 sec
    19 %
    @Temperature 71.6 °F,
    Time 70.0 hour
    ISO 815
     27 %
    @Temperature 70.0 °C,
    Time 86400 sec
    27 %
    @Temperature 158 °F,
    Time 24.0 hour
    ISO 815
     
    Thermal PropertiesMetricEnglishComments
    Vicat Softening Point 135 °C275 °FA50; ISO 306

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane
    Lubrizol Estane® 58070 Thermoplastic Polyurethane
    Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane
    Lubrizol ESTANE® 5799 Ester Based Thermoplastic Polyurethane
    Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane

    PNOVEON104 / 55371

    Polyurethane

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.