MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: Fast cycling, broad temperature performance, and durability

Use: Injection Molding.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/inflex bar
 0.010 cm/cm0.010 in/indisk
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 47 - 53
@Time 5.00 sec
47 - 53
@Time 0.00139 hour
ASTM D2240
Tensile Strength 41.0 MPa5950 psiASTM D412
Elongation at Break 450 %450 %ASTM D412/D638
100% Modulus 11.0 MPa
@Strain 100 %
1600 psi
@Strain 100 %
ASTM D412
Flexural Modulus 0.0900 GPa13.1 ksiASTM D790
Tear Strength 42.1 kN/m240 pliTrouser; ASTM D470
Graves Tear Strength 138 kN/m790 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 6262CS-17, 1000g; ASTM D3389 B
Compression Set  34 %
@Temperature 23.0 °C,
Time 79200 sec
34 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
 43 %
@Temperature 70.0 °C,
Time 79200 sec
43 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 °C424 °FDSC
Glass Transition Temp, Tg -40.0 °C-40.0 °FDSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 204 °C399 °FInjection
Middle Barrel Temperature 210 °C410 °FInjection
Front Barrel Temperature 218 °C424 °FInjection
Nozzle Temperature 223 °C433 °FInjection
Melt Temperature 223 °C433 °FInjection
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiInjection
Hold Pressure 34.5 - 68.9 MPa5000 - 10000 psiInjection
Back Pressure >= 0.345 MPa>= 50.0 psiInjection
Screw Speed 60 - 100 rpm60 - 100 rpmInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane
Delrin Delrin® 500P NC010 POM
Delrin Delrin® 100P NC010 POM
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane

PNOVEON021 / 55287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.