MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MPIF CZ-0010-U P/M Brass
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: MPIF Suffix (-U) is determined by density, which heavily influences property values.

Key Words: Power Metallurgy PM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.60 - 8.00 g/cc0.275 - 0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell H 7070
Tensile Strength, Ultimate 186 MPa27000 psi
Tensile Strength, Yield 68.9 MPa
@Strain 0.2 %
10000 psi
@Strain 0.2 %
Elongation at Break 18 %18 %in 25 mm (1 in.)
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 90 %90 %As Balance
Zinc, Zn 10 %10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Medium-leaded brass, UNS C35000, OSO50 Temper rod
Overview of materials for Brass
Phosphor bronze 5% Sn, UNS C51000, H02 Temper 25 mm rod
Copper, UNS C26800 (Yellow brass), H00 (6%) Temper rod
Copper, Cu; Cold-Worked

MCUPM104 / 193463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.