MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Medium-leaded brass, UNS C35000, OSO50 Temper rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Fair cold workability, poor hot formability.

Applications: bearing cages, book dies, clock plates, engraving plates, gears, hinges, hose couplings, keys, lock parts, lock tumblers, meter parts, nuts, sink strainers, strike plates, templates, type characters, washers, wear plates.

Test specimen: rod - 12mm diameter.

Key Words: CZ129, ISO CuZn37Pb1, ISO CuZn38Pb1, CEN CW605N, CEN CW607N
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.47 g/cc0.306 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 6565
Hardness, Rockwell 30T 2525
Tensile Strength, Ultimate 330 MPa47900 psi
Tensile Strength, Yield 110 MPa
@Strain 0.5 %
16000 psi
@Strain 0.5 %
Elongation at Break 56 %
@Diameter 12.0 mm
56 %
@Diameter 0.472 in
In 50 mm, Rod
Modulus of Elasticity 105 GPa15200 ksi
Poissons Ratio 0.3460.346
Machinability 70 %70 %UNS C36000 (free-cutting brass) = 100%
Forgeability 50 %50 %UNS C37700 (forging brass) = 100%
Shear Modulus 39.0 GPa5660 ksi
Shear Strength 235 MPa34100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
0.00000660 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.3 µm/m-°C
@Temperature 20.0 - 300 °C
11.3 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
798 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 895 - 915 °C1640 - 1680 °F
Solidus 895 °C1640 °F
Liquidus 915 °C1680 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 600 °C797 - 1110 °F
Hot-Working Temperature 760 - 800 °C1400 - 1470 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 59 - 64 %59 - 64 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb 0.80 - 1.4 %0.80 - 1.4 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn 36.4 %36.4 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Medium-leaded brass, UNS C35000, H01 Temper rod
Overview of materials for Brass
Medium-leaded brass, UNS C34000, OSO25 Temper rod
Phosphor bronze 5% Sn, UNS C51000, H02 Temper 25 mm rod
Cartridge Brass, UNS C26000 (260 Brass), OS100 Temper flat products

MC35000c2 / 11228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.