MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Medium-leaded brass, UNS C35000, OSO50 Temper rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Fair cold workability, poor hot formability.

Applications: bearing cages, book dies, clock plates, engraving plates, gears, hinges, hose couplings, keys, lock parts, lock tumblers, meter parts, nuts, sink strainers, strike plates, templates, type characters, washers, wear plates.

Test specimen: rod - 12mm diameter.

Key Words: CZ129, ISO CuZn37Pb1, ISO CuZn38Pb1, CEN CW605N, CEN CW607N
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.47 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 65
Hardness, Rockwell 30T 25
Tensile Strength, Ultimate 330 MPa
Tensile Strength, Yield 110 MPa
@Strain 0.5 %
Elongation at Break 56 %
@Diameter 12.0 mm
In 50 mm, Rod
Modulus of Elasticity 105 GPa
Poissons Ratio 0.346
Machinability 70 %UNS C36000 (free-cutting brass) = 100%
Forgeability 50 %UNS C37700 (forging brass) = 100%
Shear Modulus 39.0 GPa
Shear Strength 235 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.3 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
Melting Point 895 - 915 °C
Solidus 895 °C
Liquidus 915 °C
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 600 °C
Hot-Working Temperature 760 - 800 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 59 - 64 %
Iron, Fe <= 0.10 %
Lead, Pb 0.80 - 1.4 %
Other, total <= 0.50 %
Zinc, Zn 36.4 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Medium-leaded brass, UNS C35000, H01 Temper rod
Overview of materials for Brass
Medium-leaded brass, UNS C34000, OSO25 Temper rod
Phosphor bronze 5% Sn, UNS C51000, H02 Temper 25 mm rod
Cartridge Brass, UNS C26000 (260 Brass), OS100 Temper flat products

MC35000c2 / 11228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.