MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Struktol CALCIUM STEARATE GR
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes: High purity, non-wettable, calcium stearate granule.

STRUKTOL® Calcium Stearate GR is an effective processing aid and release agent. The low chloride content of STRUKTOL® Calcium Stearate GR allows for complete product dispersion in elastomers.
STRUKTOL® Calcium Stearate GR reduces extruder pressure build-up of rigid PVC compounds when used as a processing aid during the manufacture of pipe, siding and injection molded fittings.
The low chloride content of STRUKTOL® Calcium Stearate GR meets the quality and processing demands of polyolefin, polystyrene and polyester manufacture.
Some of the benefits of using STRUKTOL® Calcium Stearate GR are:
- LOW DUST Controlled granule size during manufacture virtually eliminates work area dust problems. - EASY HANDLING Eliminates bridging or caking while facilitating use in any type of packaging, bulk handling or conveying system. - LOW IMPURITY
Reduces extruder pressure build-up and minimizes fiber breakage during extrusion and spinning. - COLOR STABILITY
High-purity and a unique manufacturing process give this product extreme heat resistance to prevent discoloration and haze formation.

FDA Status: 173.340; 175.105; 175.300; 175.320; 176.170; 176.200; 176.210; 177.1200; 177.2260; 177.2410; 177.2600; 178.2010; 181.29; 184.1229

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/cc
Additive Loading 0.30 - 3.0 %parts
Ash 10.5 %
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 155 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 2.5 %
 
Descriptive Properties
AppearanceGranule
Free Fatty Acid (%, max)1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Struktol TR 121 Slip Agent, Lubricant, Mold Release Agent
Struktol TR 071 Processing Additive
Struktol TR 065 Blending Aid, Processing Additive
Struktol TPW 604 Processing Additive
Struktol MONTAN WAX E Lubricant, Processing Additive

PSTRUK15 / 69243

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.