Master Bond MB600SCN is an aqueous based, sodium silicate system with a silver coated nickel filler. It is intended for use in applications where very good shielding effectiveness is required and cost considerations might be more pronounced. Electromagnetic interference (EMI) and radio frequency interference (RFI) are very important factors in electronic applications. The energy emitted from various sources such as radios, appliances, etc. can interfere with other electronic devices that are made from plastics. Conductive coatings are often applied to the housings in order to protect the devices from these types of interferences. Key Features - Very good shielding effectiveness
- Temperature resistance up to +700°F
- Easy application
- Silver coated nickel filler
- Cost effective
Information provided by MasterBond® |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |