MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond FL901S One Component, Silver Filled Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Electrically conductive
  • Convenient handling
  • Good storage stability
  • Fast curing
  • Excellent physical properties
  • Uniform bond line thickness
Product Description: Master Bond FL901S is a high performance silver filled epoxy based film which offers outstanding performance properties combined with easy handling, simple processing and convenient storage stability. Unlike most electrically conductive film systems, FL901S does not require freezing, and simple refrigeration is fine. Its physical properties are particularly appealing. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics, many rubbers and plastics. It has exceptional capabilities of withstanding aggressive thermal cycling as well as thermal and mechanical shocks. FL901S has good chemical resistance especially to oils, water, etc. Its cure is straightforward and to the point, 1 hour at 250°F or 40-45 minutes at 300°F. Its service temperature range is highly commendable at -100°F to +400°F and, of course, it has extraordinary electrical conductivity; the volume resistivity being less than 1 milliohm-cm. Master Bond FL901S is available in two standard sizes. The first is 6” long x 2” wide x 0.003“ thick. The second size is 8” long x 4.3” wide x 0.003” thick. Most importantly, other sheet sizes are available as well, or it can be cut into various dimensions. Since it contains silver, it is a superb thermal conductor. FL901S cures in a manner that ensures uniform bond line thicknesses. FL901S can be used in a wide array of electronic applications for bonding, sealing and coating. It has even been used for EMI/RFI shielding. In actuality, FL901S’ versatility enables it to be used in many specialty applications where easy processing, electrical conductivity and remarkable physical characteristics are desirable.

Product Advantages:

  • Film system, no mixing required. Provides for uniform bond line thicknesses
  • Simple heat curing at 250-300°F
  • Magnificent electrical conductivity
  • Available in convenient shapes and sizes; specialty preforms are available
  • Exemplary thermal cycling capabilities
  • Dependable adhesion to a wide variety of substrates

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus >= 2.07 GPa>= 300 ksi
Adhesive Bond Strength >= 8.27 MPa>= 1200 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00020 ohm-cm<= 0.00020 ohm-cm
Dielectric Constant 4.1
@Frequency 60 Hz
4.1
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 75.0 - 85.0 µm/m-°C41.7 - 47.2 µin/in-°F
Thermal Conductivity 2.02 - 2.16 W/m-K14.0 - 15.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg 85.0 °C185 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  45.0 min
@Temperature 149 °C
0.750 hour
@Temperature 300 °F
 60.0 min
@Temperature 121 °C
1.00 hour
@Temperature 250 °F
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
6.00 Month
@Temperature 40.0 - 50.0 °F
in original, unopened containers
 
Descriptive Properties
Colorsliver/gray
Composition<60 ppmTotal ionic impurities (chloride, sodium, potassium)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding
Master Bond FLM36 B-staged film for high performance bonding and sealing
Master Bond FL901AO One Component Thermally Conductive Epoxy Adhesive Film
Master Bond MasterSil 151AO Thermally Conductive Silicone System

PMASTM916 / 185509

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.