MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Master Bond MasterSil 705C is an electrically conductive, one component, non-corrosive, carbon filled silicone for bonding, sealing and coating. This black colored paste like system cures readily at ambient temperatures upon exposure to humidity; the higher the level, the faster the rate of cure. MasterSil 705C has good electrical conductivity and is used primarily in applications involving static dissipation or EMI-RFI shielding. MasterSil 705C is also used when an electrically conductive system that is non-metallic is required. It retains typical silicone type flexibility and high temperature resistance. It is serviceable over the wide temperature range of -75°F to +400°F. MasterSil 705C will bond well to a wide variety of substrates including other silicone materials, particularly gasket materials. It is most effective when applied in thin sections. Another highly desirable property is a very fast tack free time of 3-7 minutes depending upon humidity.

Key Features

  • Carbon filled
  • Electrically conductive
  • Room temperature curing
  • Serviceable from -75°F to +400°F

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
Tensile Strength at Break 1.72 MPa250 psi
Elongation at Break 230 %230 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 50 - 100 ohm-cm50 - 100 ohm-cm
Dielectric Constant 4.2
@Frequency 50 Hz,
Temperature 25.0 °C
4.2
@Frequency 50 Hz,
Temperature 77.0 °F
Dielectric Strength 33.5 kV/mm850 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Tack-Free Time 3.00 - 7.00 min0.0500 - 0.117 hour
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original unopened containers
 
Descriptive Properties
Appearanceblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Master Bond FL901AO One Component Thermally Conductive Epoxy Adhesive Film
Master Bond FL901S One Component, Silver Filled Epoxy
Master Bond FLM36 B-staged film for high performance bonding and sealing

PMASTB337 / 149584

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.