MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP-105 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar surfaces where thermal coefficient of expansion may be a problem. It is also unique in that it retains its clear, colorless properties even when cured in larger masses where many clear epoxy systems will often turn amber from the reaction exotherm.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 1000 - 5000 cPBase, RVF #7 spindle, 20 rpm @ 27°C
 8000 - 16000 cPAccelerator, RVF #7 spindle, 20 rpm @ 27°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 39ASTM D2240
Tensile Strength at Break 4.14 MPaASTM D882
Elongation at Break 120 %ASTM D882
Shear Strength 80.0 psiOverlap, Polypropylene
 200 psiOverlap, Glass, Borosilicate
 250 psiOverlap, +3M Primer 3901
 250 psiOverlap, Acrylic
 300 psiOverlap, Wood, Fir
 300 psiOverlap, ABS
 400 psiOverlap, Polycarbonate
 520 psiOverlap, PVC
 1300 psiOverlap, Cold Rolled Steel
 1400 psiOverlap, Fiberglass
 1500 psiOverlap, Sanded Aluminum
 2000 psiOverlap, Etched Aluminum
 150 psi
@Temperature 82.0 °C
Overlap
 250 psi
@Temperature 66.0 °C
Overlap
 400 psi
@Temperature 49.0 °C
Overlap
 2000 psi
@Temperature 21.0 °C
Overlap
 3500 psi
@Temperature -53.0 °C
Overlap
Peel Strength 1.00 pli180°
 2.00 pli180°
 3.00 pli180°
 5.00 pli180°
 35.0 pli180°
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+10 ohm-cmASTM D257
Dielectric Constant 9.2
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 465 kV/in
@Thickness 0.762 mm
ASTM D149
Dissipation Factor 0.22
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 181 µm/m-°C
@Temperature 40.0 - 140 °C
Thermal Conductivity 0.147 W/m-K
@Temperature 44.3 °C
ASTM C177
Glass Transition Temp, Tg 8.00 °COnset
 15.0 °CMid-Point
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 minHandling Strength
 48.0 hour
Tack-Free Time 10.0 min
 
Descriptive Properties
AppearanceClearBase
 ClearAccelerator
 Clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M Scotch-Weld™ DP-125 Translucent Adhesive in Duo-Pak Cartridges
3M Scotch-Weld™ DP-105 Clear Adhesive in Duo-Pak Cartridges
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
3M Scotch-Weld™ DP-100 Plus Clear Adhesive in Duo-Pak Cartridges

PMM34618 / 169365

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.