Physical Properties | Metric | English | Comments |
---|
Brookfield Viscosity | 40000 - 80000 cP | 40000 - 80000 cP |
| 75000 - 150000 cP | 75000 - 150000 cP |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore D | 50 - 65 | 50 - 65 |
Shear Modulus | 0.342 GPa @Temperature 24.0 °C | 49.6 ksi @Temperature 75.2 °F |
| 1.509 GPa @Temperature 0.000 °C | 218.8 ksi @Temperature 32.0 °F |
| 1.946 GPa @Temperature -40.0 °C | 282.3 ksi @Temperature -40.0 °F |
| 2.1984 GPa @Temperature -60.0 °C | 318.85 ksi @Temperature -76.0 °F |
| 2.74 GPa @Temperature -100 °C | 398 ksi @Temperature -148 °F |
Shear Strength | 1.38 MPa | 200 psi |
| 1.52 MPa | 220 psi |
| 2.07 MPa | 300 psi |
| 3.45 MPa | 500 psi |
| 4.21 MPa | 610 psi |
| 5.86 MPa | 850 psi |
| 6.48 MPa | 940 psi |
| 6.83 MPa | 990 psi |
| 7.24 MPa | 1050 psi |
| 7.58 MPa | 1100 psi |
| 8.07 MPa | 1170 psi |
| 8.89 MPa | 1290 psi |
| 10.38 MPa | 1505 psi |
| 11.4 MPa | 1660 psi |
| 11.7 MPa | 1700 psi |
| 12.4 MPa | 1800 psi |
| 12.8 MPa | 1850 psi |
| 13.1 MPa | 1900 psi |
| 13.69 MPa | 1985 psi |
| 14.31 MPa | 2075 psi |
| 15.9 MPa | 2300 psi |
| 17.2 MPa | 2500 psi |
| 17.2 MPa | 2500 psi |
| 20.28 MPa | 2942 psi |
| 20.3 MPa | 2950 psi |
| 21.5 MPa | 3120 psi |
| 22.8 MPa | 3300 psi |
| 22.8 MPa | 3300 psi |
| 32.1 MPa | 4650 psi |
| 34.0 MPa | 4930 psi |
| 2.76 MPa @Temperature 82.0 °C | 400 psi @Temperature 180 °F |
| 16.8 MPa @Temperature -253 °C | 2440 psi @Temperature -423 °F |
| 18.9 MPa @Temperature -196 °C | 2740 psi @Temperature -321 °F |
| 20.7 MPa @Temperature -73.0 °C | 3000 psi @Temperature -99.4 °F |
| 20.7 MPa @Temperature -53.0 °C | 3000 psi @Temperature -63.4 °F |
| 22.1 MPa @Temperature 24.0 °C | 3200 psi @Temperature 75.2 °F |
| 2.90 MPa @Temperature 117 °C, Time 4.406e+6 sec | 420 psi @Temperature 243 °F, Time 1224 hour |
| 3.03 MPa @Temperature 117 °C, Time 4.406e+6 sec | 440 psi @Temperature 243 °F, Time 1224 hour |
| 3.45 MPa @Temperature 82.0 °C, Time 3.46e+6 sec | 500 psi @Temperature 180 °F, Time 960 hour |
| 3.86 MPa @Temperature 117 °C, Time 4.406e+6 sec | 560 psi @Temperature 243 °F, Time 1224 hour |
| 5.24 MPa @Temperature 82.0 °C, Time 3.46e+6 sec | 760 psi @Temperature 180 °F, Time 960 hour |
| 6.89 MPa @Temperature 82.0 °C, Time 3.46e+6 sec | 1000 psi @Temperature 180 °F, Time 960 hour |
| 7.72 MPa @Temperature 82.0 °C, Time 3.46e+6 sec | 1120 psi @Temperature 180 °F, Time 960 hour |
| 15.2 MPa @Temperature -53.0 °C, Time 0.000 sec | 2200 psi @Temperature -63.4 °F, Time 0.000 hour |
| 19.7 MPa @Temperature -53.0 °C, Time 0.000 sec | 2860 psi @Temperature -63.4 °F, Time 0.000 hour |
| 21.4 MPa @Temperature 24.0 °C, Time 1.04e+6 sec | 3100 psi @Temperature 75.2 °F, Time 288 hour |
| 21.5 MPa @Temperature -53.0 °C, Time 0.000 sec | 3120 psi @Temperature -63.4 °F, Time 0.000 hour |
| 22.8 MPa @Temperature -53.0 °C, Time 0.000 sec | 3310 psi @Temperature -63.4 °F, Time 0.000 hour |
| 32.7 MPa @Temperature 24.0 °C, Time 1.04e+6 sec | 4740 psi @Temperature 75.2 °F, Time 288 hour |
| 34.0 MPa @Temperature 24.0 °C, Time 1.04e+6 sec | 4930 psi @Temperature 75.2 °F, Time 288 hour |
| 35.5 MPa @Temperature 24.0 °C, Time 1.04e+6 sec | 5150 psi @Temperature 75.2 °F, Time 288 hour |
Peel Strength | 4.38 kN/m | 25.0 pli |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | 1.90e+12 ohm-cm | 1.90e+12 ohm-cm |
Surface Resistance | 5.50e+16 ohm | 5.50e+16 ohm |
Dielectric Constant | 6.3 @Temperature 60.0 °C | 6.3 @Temperature 140 °F |
| 5.51 @Frequency 1000 Hz, Temperature 23.0 °C | 5.51 @Frequency 1000 Hz, Temperature 73.4 °F |
Dielectric Strength | 16.1 kV/mm | 408 kV/in |
Dissipation Factor | 0.112 @Frequency 1000 Hz, Temperature 23.0 °C | 0.112 @Frequency 1000 Hz, Temperature 73.4 °F |
| 0.422 @Frequency 1000 Hz, Temperature 60.0 °C | 0.422 @Frequency 1000 Hz, Temperature 140 °F |
Arc Resistance | 130 sec | 130 sec |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 102 µm/m-°C @Temperature 0.000 - 40.0 °C | 56.7 µin/in-°F @Temperature 32.0 - 104 °F |
| 134 µm/m-°C @Temperature 40.0 - 80.0 °C | 74.4 µin/in-°F @Temperature 104 - 176 °F |
Thermal Conductivity | 0.395 W/m-K | 2.74 BTU-in/hr-ft²-°F |
|
Processing Properties | Metric | English | Comments |
---|
Cure Time | 480 - 720 min | 8.00 - 12.0 hour |
|
Descriptive Properties |
---|
Appearance | Gray |
| Gray |
| White |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.