MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it combines high shear strength with good peel performance properties. It is transparent and slightly flexible when cured.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 4000 - 11000 cP4000 - 11000 cPBase, RVF #7 spindle, 20 rpm @ 27°C
 7000 - 13000 cP7000 - 13000 cPAccelerator, RVF #7 spindle, 20 rpm @ 27°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ASTM D2240
Tensile Strength at Break 12.8 MPa1860 psiASTM D882
Elongation at Break 75 %75 %ASTM D882
Shear Strength 0.552 MPa80.0 psiOverlap, Polypropylene
 1.72 MPa250 psiOverlap, Glass, Borosilicate
 1.93 MPa280 psiOverlap, ABS
 2.07 MPa300 psiOverlap, +3M Scotch-Weld Primer EC3901
 2.07 MPa300 psiOverlap, Acrylic
 3.10 MPa450 psiOverlap, PVC
 4.14 MPa600 psiOverlap, Polycarbonate
 4.83 MPa700 psiOverlap, Wood, Fir
 10.3 MPa1500 psiOverlap, Fiberglass
 11.7 MPa1700 psiOverlap, Cold Rolled Steel
 12.4 MPa1800 psiOverlap, Sanded Aluminum
 24.1 MPa3500 psiOverlap, Etched Aluminum
 1.38 MPa
@Temperature 82.0 °C
200 psi
@Temperature 180 °F
Overlap
 2.76 MPa
@Temperature 66.0 °C
400 psi
@Temperature 151 °F
Overlap
 5.17 MPa
@Temperature 49.0 °C
750 psi
@Temperature 120 °F
Overlap
 20.7 MPa
@Temperature -55.0 °C
3000 psi
@Temperature -67.0 °F
Overlap
 24.1 MPa
@Temperature 21.0 °C
3500 psi
@Temperature 69.8 °F
Overlap
Peel Strength 0.175 kN/m1.00 pli
 0.351 kN/m2.00 pli180°
 0.351 kN/m2.00 pli180°
 2.28 kN/m13.0 pli180°
 2.63 kN/m15.0 pli180°
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.70e+11 ohm-cm6.70e+11 ohm-cmASTM D257
Dielectric Constant 6.6
@Frequency 1000 Hz
6.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 28.0 kV/mm
@Thickness 0.762 mm
710 kV/in
@Thickness 0.0300 in
ASTM D150
Dissipation Factor 0.060
@Frequency 1000 Hz
0.060
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  93.0 µm/m-°C
@Temperature 5.00 - 20.0 °C
51.7 µin/in-°F
@Temperature 41.0 - 68.0 °F
Below Tg
 182 µm/m-°C
@Temperature 40.0 - 140 °C
101 µin/in-°F
@Temperature 104 - 284 °F
Above Tg
Thermal Conductivity 0.133 W/m-K
@Thickness 6.35 mm,
Temperature 44.3 °C
0.923 BTU-in/hr-ft²-°F
@Thickness 0.250 in,
Temperature 112 °F
Glass Transition Temp, Tg 23.0 °C73.4 °FOnset
 29.0 °C84.2 °FMid-point
 
Processing PropertiesMetricEnglishComments
Cure Time 2880 min48.0 hour
Tack-Free Time 9.00 - 10.0 min0.150 - 0.167 hour
 
Descriptive Properties
AppearanceClear
 ClearBase
 ClearAccelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M Scotch-Weld™ EC2216 Structural Adhesive
3M Scotch-Weld™ DP-125 Translucent Adhesive in Duo-Pak Cartridges
3M Scotch-Weld™ DP-105 Epoxy Adhesive
3M Scotch-Weld™ DP-105 Clear Adhesive in Duo-Pak Cartridges

PMM34616 / 169363

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.