MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it combines high shear strength with good peel performance properties. It is transparent and slightly flexible when cured.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 4000 - 11000 cPBase, RVF #7 spindle, 20 rpm @ 27°C
 7000 - 13000 cPAccelerator, RVF #7 spindle, 20 rpm @ 27°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83ASTM D2240
Tensile Strength at Break 12.8 MPaASTM D882
Elongation at Break 75 %ASTM D882
Shear Strength 80.0 psiOverlap, Polypropylene
 250 psiOverlap, Glass, Borosilicate
 280 psiOverlap, ABS
 300 psiOverlap, +3M Scotch-Weld Primer EC3901
 300 psiOverlap, Acrylic
 450 psiOverlap, PVC
 600 psiOverlap, Polycarbonate
 700 psiOverlap, Wood, Fir
 1500 psiOverlap, Fiberglass
 1700 psiOverlap, Cold Rolled Steel
 1800 psiOverlap, Sanded Aluminum
 3500 psiOverlap, Etched Aluminum
 200 psi
@Temperature 82.0 °C
Overlap
 400 psi
@Temperature 66.0 °C
Overlap
 750 psi
@Temperature 49.0 °C
Overlap
 3000 psi
@Temperature -55.0 °C
Overlap
 3500 psi
@Temperature 21.0 °C
Overlap
Peel Strength 1.00 pli
 2.00 pli180°
 2.00 pli180°
 13.0 pli180°
 15.0 pli180°
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.70e+11 ohm-cmASTM D257
Dielectric Constant 6.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 710 kV/in
@Thickness 0.762 mm
ASTM D150
Dissipation Factor 0.060
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 93.0 µm/m-°C
@Temperature 5.00 - 20.0 °C
Below Tg
 182 µm/m-°C
@Temperature 40.0 - 140 °C
Above Tg
Thermal Conductivity 0.133 W/m-K
@Thickness 6.35 mm,
Temperature 44.3 °C
Glass Transition Temp, Tg 23.0 °COnset
 29.0 °CMid-point
 
Processing PropertiesOriginal ValueComments
Cure Time 48.0 hour
Tack-Free Time 9.00 - 10.0 min
 
Descriptive Properties
AppearanceClear
 ClearBase
 ClearAccelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M Scotch-Weld™ EC2216 Structural Adhesive
3M Scotch-Weld™ DP-125 Translucent Adhesive in Duo-Pak Cartridges
3M Scotch-Weld™ DP-105 Epoxy Adhesive
3M Scotch-Weld™ DP-105 Clear Adhesive in Duo-Pak Cartridges

PMM34616 / 169363

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.