MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott P-SF69 723292.293, Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes:

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.93 g/cc0.106 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 612612HK (0.1/20)
Modulus of Elasticity 96.0 GPa13900 ksi
Poissons Ratio 0.2510.251
Shear Modulus 38.4 GPa5570 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.00 µm/m-°C
@Temperature -20.0 - 70.0 °C
5.00 µin/in-°F
@Temperature -4.00 - 158 °F
 11.1 µm/m-°C
@Temperature 30.0 - 200 °C
6.17 µin/in-°F
@Temperature 86.0 - 392 °F
Specific Heat Capacity 0.820 J/g-°C0.196 BTU/lb-°F
Thermal Conductivity 1.12 W/m-K7.77 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 508 °C946 °F
Softening Point 602 °C1120 °Fviscosity of 107.6 cP
Annealing Point 508 °C946 °Fviscosity of 1013 cP
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.674
@Wavelength 2323.4 nm
1.674
@Wavelength 2323.4 nm
 1.68
@Wavelength 1970.1 nm
1.68
@Wavelength 1970.1 nm
 1.687
@Wavelength 1529.6 nm
1.687
@Wavelength 1529.6 nm
 1.697
@Wavelength 1060 nm
1.697
@Wavelength 1060 nm
 1.698
@Wavelength 1014 nm
1.698
@Wavelength 1014 nm
 1.703
@Wavelength 852.1 nm
1.703
@Wavelength 852.1 nm
 1.711
@Wavelength 706.5 nm
1.711
@Wavelength 706.5 nm
 1.715
@Wavelength 656.3 nm
1.715
@Wavelength 656.3 nm
 1.716
@Wavelength 643.8 nm
1.716
@Wavelength 643.8 nm
 1.717
@Wavelength 632.8 nm
1.717
@Wavelength 632.8 nm
 1.722
@Wavelength 589.3 nm
1.722
@Wavelength 589.3 nm
 1.722
@Wavelength 587.6 nm
1.722
@Wavelength 587.6 nm
 1.72833
@Wavelength 546.1 nm
1.72833
@Wavelength 546.1 nm
 1.74
@Wavelength 486.1 nm
1.74
@Wavelength 486.1 nm
 1.741
@Wavelength 480 nm
1.741
@Wavelength 480 nm
 1.755
@Wavelength 435.8 nm
1.755
@Wavelength 435.8 nm
 1.768
@Wavelength 404.7 nm
1.768
@Wavelength 404.7 nm
Abbe Number 2929ve
 29.2329.23vd
Optical Dispersion 0.0247180.024718nf - nc
 0.0251160.025116nf' - nc'
Transmission, Visible  84 %
@Thickness 25.0 mm,
Wavelength 436 nm
84 %
@Thickness 0.984 in,
Wavelength 436 nm
 91 %
@Thickness 25.0 mm,
Wavelength 420 nm
91 %
@Thickness 0.984 in,
Wavelength 420 nm
 96.3 %
@Thickness 10.0 mm,
Wavelength 420 nm
96.3 %
@Thickness 0.394 in,
Wavelength 420 nm
 96.4 %
@Thickness 25.0 mm,
Wavelength 460 nm
96.4 %
@Thickness 0.984 in,
Wavelength 460 nm
 97.6 %
@Thickness 10.0 mm,
Wavelength 436 nm
97.6 %
@Thickness 0.394 in,
Wavelength 436 nm
 98.3 %
@Thickness 25.0 mm,
Wavelength 500 nm
98.3 %
@Thickness 0.984 in,
Wavelength 500 nm
 98.5 %
@Thickness 10.0 mm,
Wavelength 460 nm
98.5 %
@Thickness 0.394 in,
Wavelength 460 nm
 99.2 %
@Thickness 25.0 mm,
Wavelength 546 nm
99.2 %
@Thickness 0.984 in,
Wavelength 546 nm
 99.3 %
@Thickness 25.0 mm,
Wavelength 620 nm
99.3 %
@Thickness 0.984 in,
Wavelength 620 nm
 99.3 %
@Thickness 10.0 mm,
Wavelength 500 nm
99.3 %
@Thickness 0.394 in,
Wavelength 500 nm
 99.3 %
@Thickness 25.0 mm,
Wavelength 660 nm
99.3 %
@Thickness 0.984 in,
Wavelength 660 nm
 99.4 %
@Thickness 25.0 mm,
Wavelength 700 nm
99.4 %
@Thickness 0.984 in,
Wavelength 700 nm
 99.4 %
@Thickness 25.0 mm,
Wavelength 580 nm
99.4 %
@Thickness 0.984 in,
Wavelength 580 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 546 nm
99.7 %
@Thickness 0.394 in,
Wavelength 546 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 660 nm
99.7 %
@Thickness 0.394 in,
Wavelength 660 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 620 nm
99.7 %
@Thickness 0.394 in,
Wavelength 620 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.8 %
@Thickness 0.394 in,
Wavelength 700 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.8 %
@Thickness 0.394 in,
Wavelength 580 nm
IR Transmittance  58 %
@Thickness 25.0 mm,
Wavelength 2500 nm
58 %
@Thickness 0.984 in,
Wavelength 2500 nm
 68 %
@Thickness 25.0 mm,
Wavelength 2325 nm
68 %
@Thickness 0.984 in,
Wavelength 2325 nm
 80.4 %
@Thickness 10.0 mm,
Wavelength 2500 nm
80.4 %
@Thickness 0.394 in,
Wavelength 2500 nm
 85.7 %
@Thickness 10.0 mm,
Wavelength 2325 nm
85.7 %
@Thickness 0.394 in,
Wavelength 2325 nm
 89 %
@Thickness 25.0 mm,
Wavelength 1970 nm
89 %
@Thickness 0.984 in,
Wavelength 1970 nm
 95.4 %
@Thickness 10.0 mm,
Wavelength 1970 nm
95.4 %
@Thickness 0.394 in,
Wavelength 1970 nm
 98.3 %
@Thickness 25.0 mm,
Wavelength 1530 nm
98.3 %
@Thickness 0.984 in,
Wavelength 1530 nm
 99.3 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99.3 %
@Thickness 0.394 in,
Wavelength 1530 nm
 99.8 %
@Thickness 25.0 mm,
Wavelength 1060 nm
99.8 %
@Thickness 0.984 in,
Wavelength 1060 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 1060 nm
99.9 %
@Thickness 0.394 in,
Wavelength 1060 nm
UV Transmittance  0.90 %
@Thickness 25.0 mm,
Wavelength 365 nm
0.90 %
@Thickness 0.984 in,
Wavelength 365 nm
 8.0 %
@Thickness 25.0 mm,
Wavelength 370 nm
8.0 %
@Thickness 0.984 in,
Wavelength 370 nm
 16 %
@Thickness 10.0 mm,
Wavelength 365 nm
16 %
@Thickness 0.394 in,
Wavelength 365 nm
 36.4 %
@Thickness 10.0 mm,
Wavelength 370 nm
36.4 %
@Thickness 0.394 in,
Wavelength 370 nm
 39 %
@Thickness 25.0 mm,
Wavelength 380 nm
39 %
@Thickness 0.984 in,
Wavelength 380 nm
 66 %
@Thickness 25.0 mm,
Wavelength 390 nm
66 %
@Thickness 0.984 in,
Wavelength 390 nm
 68.6 %
@Thickness 10.0 mm,
Wavelength 380 nm
68.6 %
@Thickness 0.394 in,
Wavelength 380 nm
 80 %
@Thickness 25.0 mm,
Wavelength 400 nm
80 %
@Thickness 0.984 in,
Wavelength 400 nm
 84 %
@Thickness 25.0 mm,
Wavelength 405 nm
84 %
@Thickness 0.984 in,
Wavelength 405 nm
 84.7 %
@Thickness 10.0 mm,
Wavelength 390 nm
84.7 %
@Thickness 0.394 in,
Wavelength 390 nm
 91.5 %
@Thickness 10.0 mm,
Wavelength 400 nm
91.5 %
@Thickness 0.394 in,
Wavelength 400 nm
 93.3 %
@Thickness 10.0 mm,
Wavelength 405 nm
93.3 %
@Thickness 0.394 in,
Wavelength 405 nm
 
Descriptive Properties
Acid resistance class1according to JOGIS
Stress optical coefficient2.66[10-6mm2/N]
Water resistance class1according to JOGIS
Yield point/sag temperature547°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott P-LAK35 693532.385, Optical Glass
Schott IRG 24 Infrared Chalcogenide Glass
Schott P-LASF51 8104909.458, Optical Glass
Mateck Lithium Fluoride (LiF)

CSGT9913 / 183166

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.