MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott P-LAK35 693532.385, Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes:

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.85 g/cc0.139 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 53.353.3
Alkali Class, AR 1.31.3
Stain Resistance Class, FR 5.05.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 616616HK (0.1/20)
Modulus of Elasticity 101 GPa14600 ksi
Poissons Ratio 0.2890.289
Shear Modulus 39.2 GPa5690 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.10 µm/m-°C
@Temperature -30.0 - 70.0 °C
4.50 µin/in-°F
@Temperature -22.0 - 158 °F
 9.70 µm/m-°C
@Temperature 20.0 - 300 °C
5.39 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.630 J/g-°C0.151 BTU/lb-°F
Thermal Conductivity 0.720 W/m-K5.00 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 508 °C946 °F
Softening Point 598 °C1110 °Fviscosity of 107.6 cP
Annealing Point 511 °C952 °Fviscosity of 1013 cP
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.657
@Wavelength 2323.4 nm
1.657
@Wavelength 2323.4 nm
 1.664
@Wavelength 1970.1 nm
1.664
@Wavelength 1970.1 nm
 1.671
@Wavelength 1529.6 nm
1.671
@Wavelength 1529.6 nm
 1.678
@Wavelength 1060 nm
1.678
@Wavelength 1060 nm
 1.679
@Wavelength 1014 nm
1.679
@Wavelength 1014 nm
 1.682
@Wavelength 852.1 nm
1.682
@Wavelength 852.1 nm
 1.687
@Wavelength 706.5 nm
1.687
@Wavelength 706.5 nm
 1.69
@Wavelength 632.8 nm
1.69
@Wavelength 632.8 nm
 1.69
@Wavelength 643.8 nm
1.69
@Wavelength 643.8 nm
 1.693
@Wavelength 587.6 nm
1.693
@Wavelength 587.6 nm
 1.693
@Wavelength 589.3 nm
1.693
@Wavelength 589.3 nm
 1.695
@Wavelength 656.3 nm
1.695
@Wavelength 656.3 nm
 1.696
@Wavelength 546.1 nm
1.696
@Wavelength 546.1 nm
 1.702
@Wavelength 486.1 nm
1.702
@Wavelength 486.1 nm
 1.703
@Wavelength 480 nm
1.703
@Wavelength 480 nm
 1.707
@Wavelength 435.8 nm
1.707
@Wavelength 435.8 nm
 1.715
@Wavelength 404.7 nm
1.715
@Wavelength 404.7 nm
 1.725
@Wavelength 365 nm
1.725
@Wavelength 365 nm
 1.736
@Wavelength 334.1 nm
1.736
@Wavelength 334.1 nm
Abbe Number 52.9552.95ve
 53.253.2vd
Optical Dispersion 0.0130360.013036nf - nc
 0.0131560.013156nf' - nc'
Transmission, Visible  97.7 %
@Thickness 25.0 mm,
Wavelength 420 nm
97.7 %
@Thickness 0.984 in,
Wavelength 420 nm
 98 %
@Thickness 25.0 mm,
Wavelength 436 nm
98 %
@Thickness 0.984 in,
Wavelength 436 nm
 98.5 %
@Thickness 25.0 mm,
Wavelength 460 nm
98.5 %
@Thickness 0.984 in,
Wavelength 460 nm
 99.2 %
@Thickness 25.0 mm,
Wavelength 620 nm
99.2 %
@Thickness 0.984 in,
Wavelength 620 nm
 99.2 %
@Thickness 10.0 mm,
Wavelength 420 nm
99.2 %
@Thickness 0.394 in,
Wavelength 420 nm
 99.2 %
@Thickness 25.0 mm,
Wavelength 660 nm
99.2 %
@Thickness 0.984 in,
Wavelength 660 nm
 99.2 %
@Thickness 25.0 mm,
Wavelength 500 nm
99.2 %
@Thickness 0.984 in,
Wavelength 500 nm
 99.3 %
@Thickness 25.0 mm,
Wavelength 700 nm
99.3 %
@Thickness 0.984 in,
Wavelength 700 nm
 99.3 %
@Thickness 25.0 mm,
Wavelength 580 nm
99.3 %
@Thickness 0.984 in,
Wavelength 580 nm
 99.4 %
@Thickness 25.0 mm,
Wavelength 546 nm
99.4 %
@Thickness 0.984 in,
Wavelength 546 nm
 99.4 %
@Thickness 10.0 mm,
Wavelength 436 nm
99.4 %
@Thickness 0.394 in,
Wavelength 436 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 620 nm
99.7 %
@Thickness 0.394 in,
Wavelength 620 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 460 nm
99.7 %
@Thickness 0.394 in,
Wavelength 460 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 546 nm
99.7 %
@Thickness 0.394 in,
Wavelength 546 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.7 %
@Thickness 0.394 in,
Wavelength 700 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 660 nm
99.7 %
@Thickness 0.394 in,
Wavelength 660 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.7 %
@Thickness 0.394 in,
Wavelength 580 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 500 nm
99.8 %
@Thickness 0.394 in,
Wavelength 500 nm
IR Transmittance  22 %
@Thickness 25.0 mm,
Wavelength 2500 nm
22 %
@Thickness 0.984 in,
Wavelength 2500 nm
 50 %
@Thickness 25.0 mm,
Wavelength 2325 nm
50 %
@Thickness 0.984 in,
Wavelength 2325 nm
 75.8 %
@Thickness 10.0 mm,
Wavelength 2325 nm
75.8 %
@Thickness 0.394 in,
Wavelength 2325 nm
 84.6 %
@Thickness 10.0 mm,
Wavelength 2500 nm
84.6 %
@Thickness 0.394 in,
Wavelength 2500 nm
 87 %
@Thickness 25.0 mm,
Wavelength 1970 nm
87 %
@Thickness 0.984 in,
Wavelength 1970 nm
 94.6 %
@Thickness 10.0 mm,
Wavelength 1970 nm
94.6 %
@Thickness 0.394 in,
Wavelength 1970 nm
 98.1 %
@Thickness 25.0 mm,
Wavelength 1530 nm
98.1 %
@Thickness 0.984 in,
Wavelength 1530 nm
 99.2 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99.2 %
@Thickness 0.394 in,
Wavelength 1530 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 1060 nm
99.9 %
@Thickness 0.394 in,
Wavelength 1060 nm
 99.9 %
@Thickness 25.0 mm,
Wavelength 1060 nm
99.9 %
@Thickness 0.984 in,
Wavelength 1060 nm
UV Transmittance  0.50 %
@Thickness 25.0 mm,
Wavelength 300 nm
0.50 %
@Thickness 0.984 in,
Wavelength 300 nm
 2.6 %
@Thickness 10.0 mm,
Wavelength 290 nm
2.6 %
@Thickness 0.394 in,
Wavelength 290 nm
 6.0 %
@Thickness 25.0 mm,
Wavelength 310 nm
6.0 %
@Thickness 0.984 in,
Wavelength 310 nm
 15.8 %
@Thickness 10.0 mm,
Wavelength 300 nm
15.8 %
@Thickness 0.394 in,
Wavelength 300 nm
 21 %
@Thickness 25.0 mm,
Wavelength 320 nm
21 %
@Thickness 0.984 in,
Wavelength 320 nm
 35.3 %
@Thickness 10.0 mm,
Wavelength 310 nm
35.3 %
@Thickness 0.394 in,
Wavelength 310 nm
 48 %
@Thickness 25.0 mm,
Wavelength 334 nm
48 %
@Thickness 0.984 in,
Wavelength 334 nm
 53.6 %
@Thickness 10.0 mm,
Wavelength 320 nm
53.6 %
@Thickness 0.394 in,
Wavelength 320 nm
 74 %
@Thickness 25.0 mm,
Wavelength 350 nm
74 %
@Thickness 0.984 in,
Wavelength 350 nm
 74.6 %
@Thickness 10.0 mm,
Wavelength 334 nm
74.6 %
@Thickness 0.394 in,
Wavelength 334 nm
 88 %
@Thickness 25.0 mm,
Wavelength 365 nm
88 %
@Thickness 0.984 in,
Wavelength 365 nm
 88.7 %
@Thickness 10.0 mm,
Wavelength 350 nm
88.7 %
@Thickness 0.394 in,
Wavelength 350 nm
 90.7 %
@Thickness 25.0 mm,
Wavelength 370 nm
90.7 %
@Thickness 0.984 in,
Wavelength 370 nm
 94 %
@Thickness 25.0 mm,
Wavelength 380 nm
94 %
@Thickness 0.984 in,
Wavelength 380 nm
 95 %
@Thickness 10.0 mm,
Wavelength 365 nm
95 %
@Thickness 0.394 in,
Wavelength 365 nm
 96 %
@Thickness 25.0 mm,
Wavelength 390 nm
96 %
@Thickness 0.984 in,
Wavelength 390 nm
 96.2 %
@Thickness 10.0 mm,
Wavelength 370 nm
96.2 %
@Thickness 0.394 in,
Wavelength 370 nm
 97 %
@Thickness 25.0 mm,
Wavelength 400 nm
97 %
@Thickness 0.984 in,
Wavelength 400 nm
 97.3 %
@Thickness 25.0 mm,
Wavelength 405 nm
97.3 %
@Thickness 0.984 in,
Wavelength 405 nm
 98.4 %
@Thickness 10.0 mm,
Wavelength 380 nm
98.4 %
@Thickness 0.394 in,
Wavelength 380 nm
 98.8 %
@Thickness 10.0 mm,
Wavelength 390 nm
98.8 %
@Thickness 0.394 in,
Wavelength 390 nm
 98.9 %
@Thickness 10.0 mm,
Wavelength 400 nm
98.9 %
@Thickness 0.394 in,
Wavelength 400 nm
 99.1 %
@Thickness 10.0 mm,
Wavelength 405 nm
99.1 %
@Thickness 0.394 in,
Wavelength 405 nm
 
Descriptive Properties
Acid resistance class4according to JOGIS
Climatic resistance2
Grindability119according to JOGIS
Phosphate resistance4.3
Stress optical coefficient1.76[10-6mm2/N]
Water resistance class3according to JOGIS
Yield point/sag temperature544°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott N-BK7 Glass
Schott P-SF69 723292.293, Optical Glass
Schott IRG 24 Infrared Chalcogenide Glass

CSGT9900 / 183153

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.