MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott IRG 24 Infrared Chalcogenide Glass
Categories: Ceramic; Glass; Optical; Sulfide/Chalcogenide

Material Notes: IRG 24 has excellent transmission in the SWIR, MWIR, & LWIR and has the lowest dn/dT of the IR series glasses. Physical properties such as low dn/dT and low dispersion enable optical engineers to design color corrected optical systems without thermal defocusing. IRG 24 is optimized for pairing within the family of IR glasses and with other IR materials to support cost effective and high performance optical designs. Furthermore, IRG 24 can be processed by conventional grinding and polishing, single point diamond turning, or molding to support low to high volume component level fabrication.

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.47 g/cc0.161 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 1.121.12[GPA]
Modulus of Elasticity 20.5 GPa2970 ksi
Poissons Ratio 0.2090.209Calculated
Fracture Toughness 0.347 MPa-m½0.316 ksi-in½
Shear Modulus 8.48 GPa1230 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.4 µm/m-°C11.3 µin/in-°F
Specific Heat Capacity 0.370 J/g-°C0.0884 BTU/lb-°F
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 225 °C437 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  2.604
@Wavelength 12000 nm
2.604
@Wavelength 12000 nm
 2.606
@Wavelength 11000 nm
2.606
@Wavelength 11000 nm
 2.609
@Wavelength 10000 nm
2.609
@Wavelength 10000 nm
 2.611
@Wavelength 9000 nm
2.611
@Wavelength 9000 nm
 2.613
@Wavelength 8000 nm
2.613
@Wavelength 8000 nm
 2.615
@Wavelength 7000 nm
2.615
@Wavelength 7000 nm
 2.617
@Wavelength 6000 nm
2.617
@Wavelength 6000 nm
 2.619
@Wavelength 5000 nm
2.619
@Wavelength 5000 nm
 2.622
@Wavelength 4000 nm
2.622
@Wavelength 4000 nm
 2.627
@Wavelength 3000 nm
2.627
@Wavelength 3000 nm
 2.641
@Wavelength 2000 nm
2.641
@Wavelength 2000 nm
 2.661
@Wavelength 1500 nm
2.661
@Wavelength 1500 nm
 2.724
@Wavelength 1000 nm
2.724
@Wavelength 1000 nm
 2.755
@Wavelength 900 nm
2.755
@Wavelength 900 nm
 2.803
@Wavelength 800 nm
2.803
@Wavelength 800 nm
Transmission, Visible 0.00 %
@Wavelength 750 nm
0.00 %
@Wavelength 750 nm
IR Transmittance  2.28 %
@Wavelength 13000 nm
2.28 %
@Wavelength 13000 nm
 2.41 %
@Wavelength 11500 nm
2.41 %
@Wavelength 11500 nm
 13.5 %
@Wavelength 800 nm
13.5 %
@Wavelength 800 nm
 15.02 %
@Wavelength 13500 nm
15.02 %
@Wavelength 13500 nm
 35.02 %
@Wavelength 14000 nm
35.02 %
@Wavelength 14000 nm
 48.2 %
@Wavelength 850 nm
48.2 %
@Wavelength 850 nm
 57.63 %
@Wavelength 900 nm
57.63 %
@Wavelength 900 nm
 59.77 %
@Wavelength 950 nm
59.77 %
@Wavelength 950 nm
 60.86 %
@Wavelength 8000 nm
60.86 %
@Wavelength 8000 nm
 60.95 %
@Wavelength 1000 nm
60.95 %
@Wavelength 1000 nm
 61.57 %
@Wavelength 11000 nm
61.57 %
@Wavelength 11000 nm
 61.76 %
@Wavelength 1100 nm
61.76 %
@Wavelength 1100 nm
 62.52 %
@Wavelength 1200 nm
62.52 %
@Wavelength 1200 nm
 62.99 %
@Wavelength 1300 nm
62.99 %
@Wavelength 1300 nm
 63.37 %
@Wavelength 1400 nm
63.37 %
@Wavelength 1400 nm
 63.5 %
@Wavelength 1450 nm
63.5 %
@Wavelength 1450 nm
 63.8 %
@Wavelength 10500 nm
63.8 %
@Wavelength 10500 nm
 64.03 %
@Wavelength 1550 nm
64.03 %
@Wavelength 1550 nm
 64.05 %
@Wavelength 1650 nm
64.05 %
@Wavelength 1650 nm
 64.2 %
@Wavelength 3000 nm
64.2 %
@Wavelength 3000 nm
 64.23 %
@Wavelength 1750 nm
64.23 %
@Wavelength 1750 nm
 64.26 %
@Wavelength 1850 nm
64.26 %
@Wavelength 1850 nm
 64.48 %
@Wavelength 1950 nm
64.48 %
@Wavelength 1950 nm
 64.58 %
@Wavelength 2050 nm
64.58 %
@Wavelength 2050 nm
 64.61 %
@Wavelength 2250 nm
64.61 %
@Wavelength 2250 nm
 64.62 %
@Wavelength 2150 nm
64.62 %
@Wavelength 2150 nm
 64.78 %
@Wavelength 2350 nm
64.78 %
@Wavelength 2350 nm
 64.8 %
@Wavelength 2450 nm
64.8 %
@Wavelength 2450 nm
 64.81 %
@Wavelength 2500 nm
64.81 %
@Wavelength 2500 nm
 65.84 %
@Wavelength 4500 nm
65.84 %
@Wavelength 4500 nm
 65.9 %
@Wavelength 10000 nm
65.9 %
@Wavelength 10000 nm
 65.92 %
@Wavelength 3500 nm
65.92 %
@Wavelength 3500 nm
 65.93 %
@Wavelength 8500 nm
65.93 %
@Wavelength 8500 nm
 66.1 %
@Wavelength 9500 nm
66.1 %
@Wavelength 9500 nm
 66.29 %
@Wavelength 9000 nm
66.29 %
@Wavelength 9000 nm
 66.31 %
@Wavelength 5000 nm
66.31 %
@Wavelength 5000 nm
 66.38 %
@Wavelength 4000 nm
66.38 %
@Wavelength 4000 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott P-LAK35 693532.385, Optical Glass
Schott P-SF69 723292.293, Optical Glass
Schott IRG 22 Infrared Chalcogenide Glass
Schott IRG 26 Infrared Chalcogenide Glass
Schott IRG 25 Infrared Chalcogenide Glass

CSGT9931 / 183184

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.