MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: MAGNUM™ 3325MT is a medium heat ABS. Its inherent low gloss combined with a high flow makes it specifically suitable for unpainted interior automotive applications. MAGNUM 3325MT can thereby help you to save up to 50% of the part costs. It is globally available, locally produced in major car production regions.

Benefits:

  • Lot to lot consistency allowing for optimal machine parameters setting from the start
  • Self-coloring enabling improvement of costs by using less pigments and lowering your logistic costs
  • Low VOC allowing a better interior air quality facing increasing regulatory and OEMs constraints.
  • Heat stability during wide range of processing temperatures: enhanced part design freedom
  • High scratch and mar resistance for an improved aesthetic durability of the parts
  • Easier recyclability of unpainted part.
Applications:
  • Matt/unpainted interior automotive applications
  • Mid-consoles
  • Pillars
  • Door liners
  • Glove boxes
Automotive Specifications:
  • CHRYSLER MS-DB-191 Type A CPN1497 Color: Black
  • DAIMLER DBL 5404.8
  • FORD WSK-M4D827-A
  • FORD WSS-M4D827-C1
  • GM GMW 15572P-ABS-T2
  • CHRYSLER MS-DB-191 Type A CPN1734 Color: Color Match
  • FORD ESB-M4D483-A2
  • FORD WSS-M4D483
  • GM GMP.ABS.003
  • RNPO A S31

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183/B
Apparent Bulk Density 0.650 g/ccISO 60
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 in/inISO 294-4
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 43.0 MPa
@Thickness 3.20 mm
Injection Molded; ISO 527-2/50
Elongation at Yield 3.3 %
@Thickness 3.20 mm
Injection Molded; ISO 527-2/50
Tensile Modulus 2200 MPa
@Thickness 3.20 mm
Injection Molded; ISO 527-2
Flexural Strength 65.0 MPa
@Thickness 3.20 mm
Injection Molded, 2.0 mm/min, 3-points; ISO 178
Flexural Modulus 2100 MPaInjection Molded, 2.0 mm/min, 3-points; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature -30.0 °C
Injection Molded; ISO 180/A
 17.0 kJ/m²
@Temperature 23.0 °C
Injection Molded; ISO 180/A
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -30.0 °C
Compression Molded; ISO 179/2
 11.0 kJ/m²
@Temperature -30.0 °C
Injection Molded; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
Compression Molded; ISO 179/2
 17.0 kJ/m²
@Temperature 23.0 °C
Injection Molded; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °CUnannealed; ISO 75-2/A
 101 °CAnnealed; ISO 75-2/A
Vicat Softening Point 102 °CISO 306/B50
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Descriptive Properties
Carbon Emission20 µg/gVDA 277
Fogging98 percent100°C, ISO 6452

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo PULSE™ 2100 LG PC/ABS Engineering Resin
DuPont Mobility and Materials Zytel® ST801 BK010A PA66-HI
Trinseo MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
LyondellBasell Hostacom TRC787N 600R JET BLK Thermoplastic Olefinic Elastomer
Trinseo MAGNUM™ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin

PDWST069 / 142278

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.