MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Laponite® EP Clay Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Rockwood is introducing a new grade, Laponite® EP, which is designed to give Extra Performance and enhanced rheology control under “harsh conditions”. Laponite® products are used to improve the performance and stability of a wide range of water based formulated products. Laponite® EP is a layered silicate manufactured from naturally occurring mineral sources with a proprietary organic modification. It is particularly effective in:
  • formulations with highly acidic, or with highly alkaline pH levels
  • products with higher levels of dissolved salts
  • formulas that require spray-with-cling rheology
  • systems containing higher levels of water soluble organic solvents
  • stabilizing suspensions of pigments and minerals
Application: Used for imparting a shear sensitive structure to water based systems, including household and industrial surface coatings, household and I&I cleansers, ceramic glazes and agrochemical, oilfield and horticultural products

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.900 - 1.10 g/cc0.0325 - 0.0398 lb/in³
Density 2.10 g/cc0.0759 lb/in³
pH 9.0 - 119.0 - 112% dispersion
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 10 %<= 10 %Free
 
Descriptive Properties
Color/FormFree flowing white powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Laponite® S Synthetic Layered Fluorosilicate
BYK Laponite® RDS Synthetic Layered Silicate
BYK Laponite® RD Synthetic Layered Silicate
BYK Laponite® OG Clay Additive
BYK Laponite® LV Clay Additive

PBYK062 / 185059

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.