MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling GLASGUARD Scuff and Bulkhead Liners
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: GlasGuard Scuff and Bulkhead Liners serve as a method of protecting trailer walls from damage caused by forklift trucks and careless loading and unloading of freight. Manufactured of 1/4" thick fiberglass-reinforced plastic (FRP). Offers lasting durability, no jagged edges, corrosion, rust, and moisture absorption resistance, weighs less, costs less, and fits flat. USDA approved.

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.78 g/ccASTM D-792
Water Absorption 0.30 %% by wt.; ASTM D-570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 14290 psiASTM D-638
Tensile Modulus 1.83e+6 psiASTM D-638
Flexural Strength 21770 psiASTM D-790
Flexural Modulus 1.76e+6 psiASTM D-790
Compressive Strength 38900 psiASTM D-695
Shear Strength 13400 psiASTM D-732
Izod Impact, Notched 9.80 ft-lb/inASTM D-256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 µm/m-°C
@Temperature 20.0 °C
ASTM D-696
Thermal Conductivity 0.260 W/m-KASTM C-177
 
Compliance PropertiesOriginal ValueComments
USDA Yes
 
Descriptive Properties
Standard ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Medium Alloy Steel
Röchling Glastic T-160 Fiberglass-Reinforced Polyester Laminate
Röchling Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer

PGLASX3 / 41947

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.