MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Data provided by Glastic Corporation.

NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.81 g/cc0.0654 lb/in³ASTM D792
Water Absorption 0.40 %0.40 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 54.0 MPa7830 psiASTM D638
Tensile Modulus 12.0 GPa1740 ksiASTM D638
Flexural Strength 152 MPa22000 psiASTM D790
Compressive Strength 228 MPa33100 psiASTM D695
Shear Strength 80.0 MPa11600 psiASTM D732
Izod Impact, Notched 4.80 J/cm8.99 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 3.10e+12 ohm3.10e+12 ohmInsulation Resistance, ASTM D257
Dielectric Constant  4.1
@Frequency 60 Hz
4.1
@Frequency 60 Hz
ASTM D150
 4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm457 kV/inPerpendicular, Short-term, in air; ASTM D149
Dissipation Factor  0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
ASTM D150
 0.013
@Frequency 60 Hz
0.013
@Frequency 60 Hz
ASTM D150
Arc Resistance 180 sec180 secASTM D495
Comparative Tracking Index >= 500 V>= 500 VUL746A
High Voltage Arc-Tracking Rate, HVTR 0.000 mm/min0.000 in/minUL746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.270 W/m-K1.87 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 155 °C311 °FNEMA temperature
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 160 °C320 °FUL 746B
Flammability, UL94 V-0
@Thickness >=0.800 mm
V-0
@Thickness >=0.0315 in
UL94
Oxygen Index 35 %35 %ASTM D2862

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Plywood
Röchling Glastic BMC 1401 GTP Glass-Reinforced Polyester
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade

PGLASC / 41913

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.