MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® 140 AQ Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol 140 AQ is an anionic dispersion of an aliphatic polyester urethane resin in water.

Properties / Applications: Bayhydrol 140 AQ polyurethane dispersion is suitable for many applications including adhesion promoters in metal/plastic composite structures, textile and leather coatings and primers for rigid surface coatings. The dispersion displays excellent mechanical stability. As with any product, use of Bayhydrol 140 AQ in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
Volatiles 58 - 62 %
pH 6.0 - 8.0
Viscosity 100 - 700 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 36.5 MPa
Elongation at Break 450 %
100% Modulus 5.52 MPa
@Strain 100 %
 
Processing PropertiesOriginal ValueComments
Moisture Content 60 %
 
Descriptive Properties
AppearanceMilky white liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives Chemglaze® V004 Polyurethane Coating
Covestro Bayhydrol® A 242 Polyurethane Coating
Covestro Bayhydrol® A 2227/1 Polyurethane Coating
Covestro Bayhydrol® A 2058 Polyurethane Coating
Covestro Bayhydrol® A 145 Polyurethane Coating

PCOVEST0146 / 201929

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.