MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M 9445 Adhesive Transfer Tapes with Adhesive 350
Categories: Polymer; Adhesive

Material Notes: These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strength even at elevated temperatures. These tapes are offered with a fiber reinforced adhesive which is important for roll stability in narrow widths. Tapes using adhesive 350 are designed for temperature exposure to 450°F (232°C) for short periods of time and up to 300°F (149°C) over long time frames. This adhesive is a good choice for applications which require adhesion to Low Surface Energy plastics, powder coatings and oily metals.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 5.00 mil
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 2.1875 pliH.D. Polyethylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 2.50 pliL.D. Polyethylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 5.00 pliPolypropylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 5.3125 pliABS, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 5.625 pliRigid PVC, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 6.00 pliAluminum, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 7.50 pliEpoxy, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 7.8125 pliAcrylic, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 9.0625 pliPainted Metal, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 9.0625 pliGlass, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 9.0625 pliPolycarbonate, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 9.375 pliStainless Steel, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Liner55# Densified Kraft - 3.2 mils thick

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9472 Adhesive Transfer Tapes with Adhesive 300
3M 9471LE Adhesive Transfer Tapes with Adhesive 300LSE
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9471 Adhesive Transfer Tapes with Adhesive 300

PMM33211 / 167958

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.