MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.00 - 1.65 g/ccAverage value: 1.17 g/cc Grade Count:270
Water Absorption 20.0 - 900 %Average value: 214 % Grade Count:9
Loss On Ignition 28.0 - 32.0 %Average value: 30.0 % Grade Count:5
Water Vapor Transmission 500 - 140000 g/m²/dayAverage value: 27600 g/m²/day Grade Count:12
 300 - 6500 g/m²/day
@Temperature 38.0 - 38.0 °C
Average value: 4080 g/m²/day Grade Count:4
Viscosity 72000 - 72000 cP
@Temperature 204 - 204 °C
Average value: 72000 cP Grade Count:1
Maximum Moisture Content 0.0200 - 0.0500Average value: 0.0222 Grade Count:27
Linear Mold Shrinkage 0.00110 - 0.0150 cm/cmAverage value: 0.00713 cm/cm Grade Count:95
Linear Mold Shrinkage, Transverse -0.00300 - 0.00900 cm/cmAverage value: 0.00457 cm/cm Grade Count:22
Melt Flow 3.00 - 150 g/10 minAverage value: 39.6 g/10 min Grade Count:48
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52.0 - 100Average value: 85.2 Grade Count:198
Hardness, Shore D 22.0 - 95.0Average value: 55.8 Grade Count:117
Tensile Strength, Ultimate 1.72 - 90.0 MPaAverage value: 39.7 MPa Grade Count:272
 28.42 - 51.7 MPa
@Temperature 75.0 - 75.0 °C
Average value: 39.2 MPa Grade Count:3
 28.42 - 51.7 MPa
@Time 0.000 - 4.84e+6 sec
Average value: 39.2 MPa Grade Count:3
Tensile Strength, Yield 24.7 - 33.4 MPaAverage value: 29.4 MPa Grade Count:3
Elongation at Break 30.0 - 1040 %Average value: 532 % Grade Count:275
Modulus of Elasticity 0.0200 - 2.07 GPaAverage value: 0.968 GPa Grade Count:16
Flexural Yield Strength 74.0 - 110 MPaAverage value: 95.1 MPa Grade Count:7
Flexural Modulus 0.00689 - 2.90 GPaAverage value: 0.375 GPa Grade Count:96
Resilience 35.0 - 52.0Average value: 42.7 Grade Count:7
Rebound 30.0 - 58.0 %Average value: 40.8 % Grade Count:18
Shear Modulus 0.00840 - 0.150 GPaAverage value: 0.0519 GPa Grade Count:4
 0.0138 - 0.3656 GPa
@Temperature -50.0 - 0.000 °C
Average value: 0.159 GPa Grade Count:1
Izod Impact, Notched 1.08 - 10.6 J/cmAverage value: 3.58 J/cm Grade Count:7
Izod Impact, Notched (ISO) NBGrade Count:6
 32.0 - 100 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 60.5 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) NBGrade Count:6
 42.0 - 120 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 75.8 kJ/m² Grade Count:4
Tear Strength 12.4 - 500 kN/mAverage value: 99.6 kN/m Grade Count:194
Graves Tear Strength 21.0 - 167 kN/mAverage value: 80.4 kN/m Grade Count:33
Taber Abrasion, mg/1000 Cycles 3.00 - 350Average value: 50.7 Grade Count:79
Compression Set 18.0 - 92.0 %Average value: 39.0 % Grade Count:68
Tensile Set 6.00 - 130 %Average value: 47.8 % Grade Count:50
 10.0 - 18.0 %
@Temperature 200 - 200 °C
Average value: 14.3 % Grade Count:6
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.70e+9 - 1.00e+12 ohm-cmAverage value: 3.01e+11 ohm-cm Grade Count:4
Surface Resistance 1.50e+10 - 1.00e+12 ohmAverage value: 3.04e+11 ohm Grade Count:4
Dielectric Constant 4.60 - 8.00Average value: 6.34 Grade Count:3
Dielectric Strength 39.0 - 49.0 kV/mmAverage value: 44.7 kV/mm Grade Count:3
Dissipation Factor 0.0250 - 0.121Average value: 0.0560 Grade Count:3
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:7
 
Thermal PropertiesOriginal ValueComments
CTE, linear 88.7 - 175 µm/m-°CAverage value: 153 µm/m-°C Grade Count:22
 88.7 - 170 µm/m-°C
@Temperature -80.0 - -30.0 °C
Average value: 137 µm/m-°C Grade Count:6
Melting Point 110 - 284 °CAverage value: 156 °C Grade Count:38
Maximum Service Temperature, Air 100 °CAverage value: 100 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 65.0 - 132 °CAverage value: 103 °C Grade Count:7
Vicat Softening Point 58.0 - 145 °CAverage value: 102 °C Grade Count:66
Minimum Service Temperature, Air -50.0 °CAverage value: -50.0 °C Grade Count:6
Brittleness Temperature -70.0 - -35.0 °CAverage value: -63.2 °C Grade Count:11
Glass Transition Temp, Tg -70.0 - -17.0 °CAverage value: -41.6 °C Grade Count:67
Clash Berg Stiffness Temperature -38.0 - 6.11 °CAverage value: -8.59 °C Grade Count:3
Flammability, UL94 V-2 - V-0Grade Count:9
 
Optical PropertiesOriginal ValueComments
Haze 1.00 - 23.0 %Average value: 5.61 % Grade Count:8
Transmission, Visible 90.0 %Average value: 90.0 % Grade Count:8
 
Processing PropertiesOriginal ValueComments
Processing Temperature 130 - 221 °CAverage value: 192 °C Grade Count:34
Nozzle Temperature 19.3 - 510 °CAverage value: 203 °C Grade Count:78
Adapter Temperature 138 - 224 °CAverage value: 197 °C Grade Count:99
Die Temperature 138 - 229 °CAverage value: 196 °C Grade Count:103
Melt Temperature 121 - 246 °CAverage value: 192 °C Grade Count:139
Head Temperature 190 - 200 °CAverage value: 195 °C Grade Count:4
Mold Temperature 4.40 - 95.6 °CAverage value: 32.2 °C Grade Count:98
Drying Temperature 55.0 - 110 °CAverage value: 96.7 °C Grade Count:65
Moisture Content 0.0100 - 0.100 %Average value: 0.0800 % Grade Count:8
Dew Point -40.0 - -17.8 °CAverage value: -37.4 °C Grade Count:29
Injection Pressure 2.00 - 7000 MPaAverage value: 732 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade

O5032 / 78461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.