MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NeXolve Thermalbright® C Polyimide Film
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: High performance white polyimide film.

Thermalbright® Polyimide is a high performance white polyimide film with wide ranging uses in display applications, electrical insulators, composites, industrial tapes, space structures, and many others. Thermalbright® Polyimide is useful in thermal control applications requiring low absorptivity, high emissivity, UV stability, and high temperature colorfastness.

Thermalbright® Polyimide exhibits high optical density and hiding, making it an excellent high temperature white paint replacement material. In addition to outstanding thermal and optical properties, Thermalbright® Polyimide exhibits the lowest moisture uptake of all commercially available polyimides, at 0.2%.

Thermalbright® Polyimide is available in two grades: Thermalbright® C for Electrostatic Dissipative (ESD) applications, and Thermalbright® N for applications that require electrical insulation. Continuous rolls are available now in 1 mil thickness (25 micron) and in widths up to 60 inches (152 cm).

Information Provided by NeXolve Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.95 g/ccASTM D792-08
Water Absorption 0.40 %
@Time 86400 sec
ASTM D570-98
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 79.0 MPa
@Thickness 0.0250 mm
ASTM D882-02
Elongation at Break 1.9 %
@Thickness 0.0250 mm
ASTM D882-02
Modulus of Elasticity 4.70 GPaASTM D882-02
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.00e+9 ohm-cmASTM D257-91
Surface Resistivity per Square <= 1.00e+12 ohmASTM D257-91
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.0 µm/m-°C
@Thickness 1.00 mm,
Temperature 125 - 175 °C
ASTM E831-06
Glass Transition Temp, Tg 263 °CDSC; ASTM E1356-03
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 12 %
@Thickness 0.0250 mm
Solar Transmittivity; ASTM E903-96
Emissivity (0-1) 0.77
@Thickness 1.00 mm
Infrared (Hemispherical); ASTM E408-71
Reflection Coefficient, Visible (0-1) 0.59
@Thickness 0.0250 mm
Solar Reflectivity; ASTM E903-96
 
Descriptive Properties
ApplicationsComposites
 Displays
 Electrical Insulation
 Electronics
 Insulation Blankets
 Insulation Tubing
 Paint Replacement
 Pressure Sensitive Tape
 Space Structures
 Thermal Control
CharacteristicsBright white color
 Conductive/nonconductive grades
 Extremely low moisture uptake
 High optical density
 High temperature color stability
 Printable surface
 UV resistant
 Vacuum coating compatible
Solar Absorptivity0.291 mil thickness; ASTM E903-96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NeXolve LaRC™-CP1 Polyimide
NeXolve Thermalbright® N Polyimide Film
NeXolve Clear Optionox® Polyimide Film/Coating
NeXolve UV Blocking Optionox® Polyimide Film/Coating
NeXolve White Optionox® Polyimide Film

PNEXOL906 / 171860

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.