MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NeXolve White Optionox® Polyimide Film
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: Highly UV durable with excellent weatherability and stability to ozone.

Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability to ozone. Optinox® is available in rolls up to 60” wide, or in low-temperature curing liquids for coating applications. Both the film rolls and liquid coatings are available in three grades, outlined below.

Optinox® rolls are provided either as a freestanding film, or permanently bonded to a PET backer. Additional thicknesses are also available upon request. Optinox® liquid curing resins are provided as a two-part curing system.

    Transparent Clear:
  • UV cutoff at approximately 230 nm for a 2 mm film or coating
    Transparent UV Blocking:
  • UV cutoff at approximately 395 nm for a 2 mm film or coating
    Reflective White:
  • Reflective White Film

Information Provided by NeXolve Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 48.0 MPa
@Thickness 0.0440 mm
6960 psi
@Thickness 0.00173 in
ASTM D882-02
Elongation at Break 120 %
@Thickness 0.0440 mm
120 %
@Thickness 0.00173 in
ASTM D882-02
Elongation at Yield 110 %
@Thickness 0.0440 mm
110 %
@Thickness 0.00173 in
ASTM D882-02
Modulus of Elasticity 1.30 GPa189 ksiASTM D882-02
 
Thermal PropertiesMetricEnglishComments
CTE, linear 73.0 µm/m-°C
@Thickness 1.75 mm,
Temperature -125 - 20.0 °C
40.6 µin/in-°F
@Thickness 0.0689 in,
Temperature -193 - 68.0 °F
ASTM E831-06
Glass Transition Temp, Tg 30.0 °C86.0 °FDSC; ASTM E1356-03
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 0.16 %
@Thickness 0.0440 mm
0.16 %
@Thickness 0.00173 in
Solar Transmittivity; ASTM E903-96
Reflection Coefficient, Visible (0-1) 0.74
@Thickness 1.75 mm
0.74
@Thickness 0.0689 in
Solar Reflectivity; ASTM E903-96
 
Descriptive Properties
ApplicationsComposites Protection
 Conformal Coatings
 Corrosion Resistance
CharacteristicsExtreme environment (high UV, ozone) durability
 Flexible, tough conformal coating
 Long-term terrestrial weathering protection
 Low temperature curing
Solar Absorptivity0.11.75 mil thickness; ASTM E903-96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NeXolve Clear Optionox® Polyimide Film/Coating
NeXolve Thermalbright® C Polyimide Film
NeXolve Thermalbright® N Polyimide Film
NeXolve UV Blocking Optionox® Polyimide Film/Coating
Professional Plastics Kaptrex® Polyimide Film

PNEXOL909 / 171863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.