MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NeXolve UV Blocking Optionox® Polyimide Film/Coating
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: Highly UV durable with excellent weatherability and stability to ozone.

Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability to ozone. Optinox® is available in rolls up to 60” wide, or in low-temperature curing liquids for coating applications. Both the film rolls and liquid coatings are available in three grades, outlined below.

Optinox® rolls are provided either as a freestanding film, or permanently bonded to a PET backer. Additional thicknesses are also available upon request. Optinox® liquid curing resins are provided as a two-part curing system.

    Transparent Clear:
  • UV cutoff at approximately 230 nm for a 2 mm film or coating
    Transparent UV Blocking:
  • UV cutoff at approximately 395 nm for a 2 mm film or coating
    Reflective White:
  • Reflective White Film

Information Provided by NeXolve Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 41.0 MPa
@Thickness 0.0500 mm
5950 psi
@Thickness 0.00197 in
ASTM D882-02
Elongation at Break 95 %
@Thickness 0.0500 mm
95 %
@Thickness 0.00197 in
ASTM D882-02
Elongation at Yield 74 %
@Thickness 0.0500 mm
74 %
@Thickness 0.00197 in
ASTM D882-02
Modulus of Elasticity 0.960 GPa139 ksiASTM D882-02
 
Thermal PropertiesMetricEnglishComments
CTE, linear 86.0 µm/m-°C
@Thickness 2.00 mm,
Temperature -125 - 20.0 °C
47.8 µin/in-°F
@Thickness 0.0787 in,
Temperature -193 - 68.0 °F
ASTM E831-06
Glass Transition Temp, Tg 29.0 °C84.2 °FDSC; ASTM E1356-03
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.45
@Wavelength 549 nm
1.45
@Wavelength 549 nm
Abbe; ASTM D542-00
Transmission, Visible 0.86 %
@Thickness 0.0500 mm
0.86 %
@Thickness 0.00197 in
Solar Transmittivity; ASTM E903-96
Reflection Coefficient, Visible (0-1) 0.060
@Thickness 0.0500 mm
0.060
@Thickness 0.00197 in
Solar Reflectivity; ASTM E903-96
 
Descriptive Properties
ApplicationsComposites Protection
 Conformal Coatings
 Corrosion Resistance
CharacteristicsExtreme environment (high UV, ozone) durability
 Flexible, tough conformal coating
 High optical clarity
 Long-term terrestrial weathering protection
 Low temperature curing
Solar Absorptivity0.072.0 mil thickness; ASTM E903-96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NeXolve Clear Optionox® Polyimide Film/Coating
NeXolve Thermalbright® C Polyimide Film
NeXolve Thermalbright® N Polyimide Film
NeXolve White Optionox® Polyimide Film
Professional Plastics Kaptrex® Polyimide Film

PNEXOL911 / 171865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.