MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EPICHEM Epinyl PA 66 GF 30 Polyamide 66, 30% Glass  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Characteristics: 30% glass fibre filled

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccASTM D792, ISO 1183
Water Absorption 6.0 %
@Temperature 23.0 °C
24h; ASTM D570, ISO 62
Linear Mold Shrinkage 0.0020 - 0.011 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 110ASTM D785, ISO 2039/2
Tensile Strength, Yield 170 MPaASTM D638, ISO R527
Elongation at Break 3.0 %ASTM D638, ISO R527
Flexural Strength 235 MPaASTM D790, ISO 178
Flexural Modulus 8900 MPaASTM D790, ISO 178
Izod Impact, Notched 70.0 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256, ISO 180/4a
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+13 ohmASTM D257, IEC 93
Dielectric Constant 3.5
@Frequency 1000 Hz
ASTM D150, IEC 250
Dielectric Strength 90.0 kV/mmASTM D149, IEC 243
Dissipation Factor 0.020
@Frequency 1000 Hz
ASTM D150, IEC 250
Comparative Tracking Index 475 VVDE 0303-P1, IEC 112
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C20000 h; VDE 0304/P2-1, IEC 216
 110 °C5000 h; VDE 0304/P2-1, IEC 216
 200 °Cfew hours; VDE 0304/P2-1, IEC 216
Deflection Temperature at 1.8 MPa (264 psi) 248 °CASTM D648, ISO 75
Vicat Softening Point 250 °C
@Load 5.00 kg
120°C/hr; ASTM D1525/B, ISO 306/B
 254 °C
@Load 0.999 kg
120°C/hr; ASTM D1525/A, ISO 306/A
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EPICHEM Epinyl PA 66 GF 30 H Polyamide 66, 30% Glass, Heat Stabilized
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Filled
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Filled
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Filled

PEPI010 / 82832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.