MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Vydyne R530H BK0201 is a general purpose, 30% glass-filled, heat-stabilized, high viscosity PA66 based resin designed for injection molding applications. R530H BK0201 offers standard flow with a black surface finish and maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³DAM; ISO 1183
Water Absorption 1.30 %
@Time 86400 sec
1.30 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 1.90 %1.90 %from DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00400 cm/cm
@Thickness 2.00 mm
0.00400 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.00900 cm/cm
@Thickness 2.00 mm
0.00900 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 136 MPa19700 psi50%RH; ISO 527-2
 200 MPa29000 psiDAM; ISO 527-2
Elongation at Break 3.10 %3.10 %DAM; ISO 527-2
 4.00 %4.00 %50%RH; ISO 527-2
Tensile Modulus 7.90 GPa1150 ksi50%RH; ISO 527-2
 11.0 GPa1600 ksiDAM; ISO 527-2
Flexural Strength 158 MPa22900 psi50%RH; ISO 178
 268 MPa38900 psiDAM; ISO 178
Flexural Modulus 6.40 GPa928 ksi50%RH; ISO 178
 9.40 GPa1360 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  9.40 kJ/m²
@Temperature -40.0 °C
4.47 ft-lb/in²
@Temperature -40.0 °F
50%RH; ISO 180/1A
 9.50 kJ/m²
@Temperature -30.0 °C
4.52 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 10.0 kJ/m²
@Temperature -40.0 °C
4.76 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
50%RH; ISO 180/1A
Charpy Impact Unnotched  6.60 J/cm²
@Temperature -30.0 °C
31.4 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 6.60 J/cm²
@Temperature -40.0 °C
31.4 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eU
 6.90 J/cm²
@Temperature -40.0 °C
32.8 ft-lb/in²
@Temperature -40.0 °F
50%RH; ISO 179/1eU
 7.10 J/cm²
@Temperature -30.0 °C
33.8 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 179/1eU
 7.60 J/cm²
@Temperature 23.0 °C
36.2 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
50%RH; ISO 179/1eU
Charpy Impact, Notched  0.970 J/cm²
@Temperature -40.0 °C
4.62 ft-lb/in²
@Temperature -40.0 °F
50%RH; ISO 179/1eA
 0.980 J/cm²
@Temperature -30.0 °C
4.66 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 1.00 J/cm²
@Temperature -40.0 °C
4.76 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
50%RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm
@Thickness 1.00 mm
1.00e+13 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
Dielectric Strength  28.0 kV/mm
@Thickness 1.00 mm
711 kV/in
@Thickness 0.0394 in
50%RH; IEC 60243
 40.0 kV/mm
@Thickness 1.00 mm
1020 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
Arc Resistance 60.0 - 120 sec
@Thickness 3.00 mm
60.0 - 120 sec
@Thickness 0.118 in
ASTM D 495
Comparative Tracking Index 250 - 399 V
@Thickness 3.00 mm
250 - 399 V
@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI  7.00 - 15.0 sec
@Thickness 0.750 mm
7.00 - 15.0 sec
@Thickness 0.0295 in
PLC 4; UL 746
 7.00 - 15.0 sec
@Thickness 3.00 mm
7.00 - 15.0 sec
@Thickness 0.118 in
PLC 4; UL 746
 15.0 - 30.0 sec
@Thickness 1.50 mm
15.0 - 30.0 sec
@Thickness 0.0591 in
PLC 3; UL 746
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 0.750 mm
>= 120 arcs
@Thickness 0.0295 in
PLC 0; UL 746
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
PLC 0; UL 746
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
PLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
@Thickness 3.00 mm
0.394 - 1.00 in/min
@Thickness 0.118 in
PLC 1; UL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
10.6 µin/in-°F
@Temperature 73.4 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 81.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
45.0 µin/in-°F
@Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 262 °C504 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °C496 °F50%RH, Unannealed; ISO 75-2/B
 260 °C500 °FDAM, Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 243 °C469 °F50%RH, Unannealed; ISO 75-2/A
 248 °C478 °FDAM, Unannealed; ISO 75-2/A
UL RTI, Electrical  140 °C
@Thickness 0.750 mm
284 °F
@Thickness 0.0295 in
UL 746
 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
UL 746
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  120 °C
@Thickness 0.750 mm
248 °F
@Thickness 0.0295 in
UL 746
 120 °C
@Thickness 1.50 mm
248 °F
@Thickness 0.0591 in
UL 746
 120 °C
@Thickness 3.00 mm
248 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  125 °C
@Thickness 0.750 mm
257 °F
@Thickness 0.0295 in
UL 746
 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
UL 746
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
UL 94
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
UL 94
Flame Spread 0.000 mm/min
@Thickness 2.00 mm
0.000 in/min
@Thickness 0.0787 in
ISO 3795
Glow Wire Ignition Temperature  700 °C
@Thickness 0.750 mm
1290 °F
@Thickness 0.0295 in
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
1290 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  675 °C
@Thickness 0.750 mm
1250 °F
@Thickness 0.0295 in
IEC 60695-2-12
 675 °C
@Thickness 1.50 mm
1250 °F
@Thickness 0.0591 in
IEC 60695-2-12
 675 °C
@Thickness 3.00 mm
1250 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Middle Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Front Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Nozzle Temperature 280 - 310 °C536 - 590 °FInjection
Melt Temperature 285 - 305 °C545 - 581 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA012G30
 ASTM, D6779 PA012G30
 RoHS Compliant
AppearanceBlack
Automotive Material SpecificationAisin TO20141124 - P-PA66-GF30-807
 BMW GS 93016
 CATL MS-00000037 – PA66-GF30-X-I02
 Chery Motor Q-SQR.S1-33-2012 CMP.PA66.G6
 Denso MSR-21-001
 Ford WSS-M4D752-B1
 GM GMW16270P-PA66-GF30
 GM GMW3038P-PA66-GF30H
 GM GMW3038P-PA66-GF30J
 HMG MS211-47 Type 2A
 Li Auto QLiA53100058
 Mahle SD2-181 (AR.06576) Rev. 7
 Mercedes-Benz DBL 5409 (compliance)
 Mercedes-Benz DBL5406-PV21 (compliance)
 Modine GM0280-A/B
 PSA Peugeot-Cotroën FTM64 0046
 Renault AS26
 Tesla TM-1006 v3 - 101130
 Tesla TM-1006 v3 - 201130
 Tesla TM-1006 v3 - 301130
 Toyota TSM5603G, Class 2B, Rev 5 (compliance)
 Valeo NVB 15007 Class 2B
 Valeo NVB 15007 Class 3A
 Valeo NVB 15008 Class 3
 Valeo NVB 15009 Class 3
 VW PV 1015 (compliance)
 VW PV 3936 (compliance)
 VW TL 52682 (compliance)
FeaturesAntifreeze Resistant
 Chemical Resistant
 Fatigue Resistant
 Gasoline Resistant
 Good Flow
 Heat Stabilized
 Hydrolysis Resistant
 Lubricated
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Crastin® 6129 NC010 PBT
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled
Ascend Performance Materials Vydyne® R530H NT Nylon 66, 30% Glass Filled
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Filled
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Filled

PASCE9797 / 220900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.