Physical Properties | Metric | English | Comments |
---|
Density | 1.40 g/cc | 0.0506 lb/in³ |
Water Absorption | 0.80 % @Temperature 23.0 °C, Time 86400 sec | 0.80 % @Temperature 73.4 °F, Time 24.0 hour |
Moisture Absorption at Equilibrium | 1.7 % @Temperature 23.0 °C | 1.7 % @Temperature 73.4 °F |
Linear Mold Shrinkage, Flow | 0.0040 cm/cm @Thickness 2.00 mm | 0.0040 in/in @Thickness 0.0787 in |
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 2.00 mm | 0.0090 in/in @Thickness 0.0787 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 145 MPa @Temperature 23.0 °C | 21000 psi @Temperature 73.4 °F |
| 205 MPa @Temperature 23.0 °C | 29700 psi @Temperature 73.4 °F |
Elongation at Break | 3.0 % @Temperature 23.0 °C | 3.0 % @Temperature 73.4 °F |
| 5.0 % @Temperature 23.0 °C | 5.0 % @Temperature 73.4 °F |
Tensile Modulus | 7.90 GPa @Temperature 23.0 °C | 1150 ksi @Temperature 73.4 °F |
| 10.6 GPa @Temperature 23.0 °C | 1540 ksi @Temperature 73.4 °F |
Flexural Strength | 200 MPa @Temperature 23.0 °C | 29000 psi @Temperature 73.4 °F |
| 290 MPa @Temperature 23.0 °C | 42100 psi @Temperature 73.4 °F |
Flexural Modulus | 6.50 GPa @Temperature 23.0 °C | 943 ksi @Temperature 73.4 °F |
| 10.2 GPa @Temperature 23.0 °C | 1480 ksi @Temperature 73.4 °F |
Poissons Ratio | 0.40 @Temperature 23.0 °C | 0.40 @Temperature 73.4 °F |
Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C | 4.76 ft-lb/in² @Temperature -22.0 °F |
| 12.0 kJ/m² @Temperature -30.0 °C | 5.71 ft-lb/in² @Temperature -22.0 °F |
| 12.0 kJ/m² @Temperature 23.0 °C | 5.71 ft-lb/in² @Temperature 73.4 °F |
| 14.0 kJ/m² @Temperature 23.0 °C | 6.66 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C | 33.3 ft-lb/in² @Temperature -22.0 °F |
| 8.00 J/cm² @Temperature 23.0 °C | 38.1 ft-lb/in² @Temperature 73.4 °F |
| 8.50 J/cm² @Temperature -30.0 °C | 40.4 ft-lb/in² @Temperature -22.0 °F |
| 9.00 J/cm² @Temperature 23.0 °C | 42.8 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C | 4.76 ft-lb/in² @Temperature -22.0 °F |
| 1.10 J/cm² @Temperature 23.0 °C | 5.23 ft-lb/in² @Temperature 73.4 °F |
| 1.20 J/cm² @Temperature -30.0 °C | 5.71 ft-lb/in² @Temperature -22.0 °F |
| 1.40 J/cm² @Temperature 23.0 °C | 6.66 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | 1.00e+13 ohm-cm @Thickness 1.00 mm | 1.00e+13 ohm-cm @Thickness 0.0394 in |
Dielectric Strength | 20.0 kV/mm @Thickness 1.00 mm | 508 kV/in @Thickness 0.0394 in |
Arc Resistance | 60 - 120 sec @Thickness 3.00 mm | 60 - 120 sec @Thickness 0.118 in |
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm | 250 - 399 V @Thickness 0.118 in |
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm | 7.0 - 15 sec @Thickness 0.0295 in |
| 7.0 - 15 sec @Thickness 3.00 mm | 7.0 - 15 sec @Thickness 0.118 in |
| 15 - 30 sec @Thickness 1.50 mm | 15 - 30 sec @Thickness 0.0591 in |
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm | >= 120 arcs @Thickness 0.0295 in |
| >= 120 arcs @Thickness 1.50 mm | >= 120 arcs @Thickness 0.0591 in |
| >= 120 arcs @Thickness 3.00 mm | >= 120 arcs @Thickness 0.118 in |
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min @Thickness 3.00 mm | 0.394 - 1.00 in/min @Thickness 0.118 in |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C | 11.7 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
CTE, linear, Transverse to Flow | 110 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C | 61.1 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
Melting Point | 260 °C | 500 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 260 °C | 500 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F |
UL RTI, Electrical | 140 °C @Thickness 0.750 mm | 284 °F @Thickness 0.0295 in |
| 140 °C @Thickness 1.50 mm | 284 °F @Thickness 0.0591 in |
| 140 °C @Thickness 3.00 mm | 284 °F @Thickness 0.118 in |
UL RTI, Mechanical with Impact | 125 °C @Thickness 0.750 mm | 257 °F @Thickness 0.0295 in |
| 125 °C @Thickness 1.50 mm | 257 °F @Thickness 0.0591 in |
| 125 °C @Thickness 3.00 mm | 257 °F @Thickness 0.118 in |
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.750 mm | 284 °F @Thickness 0.0295 in |
| 140 °C @Thickness 1.50 mm | 284 °F @Thickness 0.0591 in |
| 140 °C @Thickness 3.00 mm | 284 °F @Thickness 0.118 in |
Flammability, UL94 | HB @Thickness 0.750 mm | HB @Thickness 0.0295 in |
| HB @Thickness 1.50 mm | HB @Thickness 0.0591 in |
| HB @Thickness 3.00 mm | HB @Thickness 0.118 in |
Glow Wire Ignition Temperature | 725 °C @Thickness 1.50 mm | 1340 °F @Thickness 0.0591 in |
| 750 °C @Thickness 0.750 mm | 1380 °F @Thickness 0.0295 in |
| 750 °C @Thickness 3.00 mm | 1380 °F @Thickness 0.118 in |
Glow Wire Flammability Index | 700 °C @Thickness 1.50 mm | 1290 °F @Thickness 0.0591 in |
| 725 °C @Thickness 0.750 mm | 1340 °F @Thickness 0.0295 in |
| 875 °C @Thickness 3.00 mm | 1610 °F @Thickness 0.118 in |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F |
Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F |
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F |
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F |
Melt Temperature | 285 - 305 °C | 545 - 581 °F |
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F |
Drying Temperature | 80.0 °C | 176 °F |
Dry Time | 4.00 hour | 4.00 hour |
|
Descriptive Properties |
---|
Additive | Heat Stabilizer |
| Lubricant |
Agency Ratings | ASTM, D4066 PA012G35 |
| ASTM, D6779 PA012G35 |
| SAE, J1639 PA1116 |
Color | Black |
Features | Good Flow |
| Good Mold Release |
| Heat Stabilized |
| High Rigidity |
| High Strength |
| Hydrolysis Resistant |
| Lubricated |
Forms | Pellets |
Processing Method | Injection Molding |
Region | Asia Pacific |
| Europe |
| North America |
UL File Number | E70062 |
Uses | Automotive Applications |
| Automotive Under the Hood |
| Gears |
| Housings |
| Power/Other Tools |